A single side submerged arc welding arc plate, because both sides are respectively arranged in the groove through the arc plate body thickness direction of the incision, incision length and groove projection in the horizontal direction of the same length, and between the unilateral incision and groove spacing range is 20mm~30mm, therefore, when the electric arc by arc board groove, in the process of cooling shrinkage in the molten pool, can be cut to flux arc board of free shrinkage, therefore, the weld can also free shrinkage in the transverse direction, thereby greatly reducing transverse contraction stress, to control the arc end crack effect, at the same time, but also to avoid the formation of the weld seam welding pit. End forming beautiful, greatly reduce the rework repair rate, improve the welding efficiency, reduce production costs.
【技术实现步骤摘要】
一种单面埋弧焊熄弧板
本技术涉及单面埋弧焊熄弧板。
技术介绍
埋弧焊是一种电弧在焊剂层下燃烧进行焊接的方法,其固有的焊接质量稳定、焊接生产率高、无弧光及烟尘很少等优点,使其成为压力容器、管段制造、箱型梁柱登重要钢结构制造中的主要焊接方法。然而,由于在焊接时,焊缝的起弧和收弧处容易因温度等因素问题产生合金粉融合不良、气孔、焊坑、夹渣、裂纹等缺陷,因此,需要配合使用引弧板及熄弧板,以解决上述出现的问题。但是,目前的焊接方法,在使用熄弧板进行收弧时,收弧端的裂纹控制效果仍然较差,裂纹长度、深度不一,同时,在熔池冷却收缩过程中同样会产生焊坑,影响焊接质量及焊接的美观,常常需要返工修补,生产效率低,生产成本高。
技术实现思路
本技术旨在提供一种有效避免在焊缝收弧端形成焊坑及使收弧端裂纹效果好的单面埋弧焊熄弧板,使焊缝端部成型美观,大幅减少返工修补率,提高焊接工作效率,降低生产成本。本技术所述的一种单面埋弧焊熄弧板,包括熄弧板板体,熄弧板板体上设置有与待焊接板材相配合的坡口,在坡口的两侧分别设置有贯穿熄弧板板体厚度方向的切口,所述切口长度与坡口投影在水平方向上的长度相同,单侧切口与坡 ...
【技术保护点】
一种单面埋弧焊熄弧板,包括熄弧板板体(1),熄弧板板体(1)上设置有与待焊接板材相配合的坡口(2),其特征在于:在坡口(2)的两侧分别设置有贯穿熄弧板板体(1)厚度方向的切口(3),所述切口(3)长度与坡口(2)投影在水平方向上的长度相同,单侧切口(3)与坡口(2)之间的间距范围为20mm~30mm。
【技术特征摘要】
1.一种单面埋弧焊熄弧板,包括熄弧板板体(1),熄弧板板体(1)上设置有与待焊接板材相配合的坡口(2),其特征在于:在坡口(2)的两侧分别设置有贯穿熄弧板板体(1)厚度方向的切口(3),所述切口(3)长度与坡口(2)投影在水平方向上的长度相同,单侧切口(3)...
【专利技术属性】
技术研发人员:杨伟锋,兰建林,
申请(专利权)人:广州文冲船厂有限责任公司,
类型:新型