一种多焊点焊接螺母制造技术

技术编号:17133744 阅读:57 留言:0更新日期:2018-01-27 10:34
本发明专利技术涉及一种多焊点焊接螺母,包括螺母本体、圆形凸台和焊点,其技术特点在于:该螺母本体顶部沿轴向一体制出有用于定位的圆形凸台,该螺母本体和圆形凸台中心开有螺纹通孔;在圆形凸台外的螺母本体上表面上沿圆周方向均布间隔制有至少三个焊点。本发明专利技术通过将现有技术中六角焊接螺母本体上的3个焊点增加至6个焊点,焊接牢固。

A multi solder joint nut

The invention relates to a welding nut, which comprises a nut body, circular lug and solder joints, the technical characteristics that the nut at the top of the body along the axial direction are integrally made with a circular lug boss for positioning, the nut body and a circular boss is arranged in the center of a thread through hole; the nut body in a circular boss outside on the surface along the circumferential direction uniformly provided with at least three solder joints. By adding 3 solder joints on the body of the six angle welding nut in the existing technology to 6 solder joints, the welding is strong.

【技术实现步骤摘要】
一种多焊点焊接螺母
本专利技术属于紧固件
,特别是一种多焊点焊接螺母。
技术介绍
目前,在紧固件产品中,螺母因其制造工艺简单,种类繁多,被广泛认知和使用。其中,焊接螺母是指一种在螺母紧固后还需与安装板进行焊接,因此焊接螺母在普通螺母的底部端面设置有用于焊接点状凸起。但现有技术中的焊接螺母在焊接过程中存在如下问题:(1)普通的六角焊接螺母的底面端部仅制有3个焊点,焊接螺母焊接不牢,半成品件在运输过程中或转运过程中焊接螺母容易脱落。(2)现有的六角焊接螺母焊点厚度一般为0.8mm,在实际焊接作业中由于焊点高度过高,致使焊点融化速度慢,焊接效果不理想。经检索,未发现与本专利技术相同或相似的现有技术。
技术实现思路
本专利技术的目的在于克服现有技术的不足,提供一种设计合理、结构简单且焊接牢固的多焊点焊接螺母。本专利技术解决其技术问题是采取以下技术方案实现的:一种多焊点焊接螺母,包括螺母本体、圆形凸台和焊点,该螺母本体顶部沿轴向一体制出有用于定位的圆形凸台,该螺母本体和圆形凸台中心开有螺纹通孔;在圆形凸台外的螺母本体上表面上沿圆周方向均布间隔制有至少三个焊点。而且,所述多焊点螺母为六角焊接螺本文档来自技高网...
一种多焊点焊接螺母

【技术保护点】
一种多焊点焊接螺母,包括螺母本体、圆形凸台和焊点,其特征在于:该螺母本体顶部沿轴向一体制出有用于定位的圆形凸台,该螺母本体和圆形凸台中心开有螺纹通孔;在圆形凸台外的螺母本体上表面上沿圆周方向均布间隔制有至少三个焊点。

【技术特征摘要】
1.一种多焊点焊接螺母,包括螺母本体、圆形凸台和焊点,其特征在于:该螺母本体顶部沿轴向一体制出有用于定位的圆形凸台,该螺母本体和圆形凸台中心开有螺纹通孔;在圆形凸台外的螺母本体上表面上沿圆周方向均布间隔制有至少三个焊点。2.根据权利要求1所述的一种多焊点焊接螺母...

【专利技术属性】
技术研发人员:闫宝祥吕占军赵月起李树干徐秀腾
申请(专利权)人:天津市天龙得冷成型部件有限公司
类型:发明
国别省市:天津,12