The invention discloses a preparation method of de olefin catalyst, the de olefin catalyst includes: rare earth metal oxide particles, which is characterized in that the particles also contain active substances, and the weight of the particles accounted for 90 of the total weight of the two 99.9%. Active material weight accounted for 0.1 of the total weight of the two 10%; the preparation method is de olefin catalyst impregnation method comprises: dipping, drying and screening finished each process step. Compared with the prior art, the present invention has the following advantages: because the particles contain active substances, the catalyst has better catalytic activity, so that the consumption can be obviously reduced in use. The experimental results show that the treatment of 1 tons of aromatic hydrocarbons containing unsaturated olefins requires the use of 1Kg products, thereby significantly reducing the production cost of aromatic hydrocarbons.
【技术实现步骤摘要】
一种脱烯烃催化剂的制备方法
本专利技术设计一种化工产品的制备方法,确切地说是一种脱烯烃催化剂的制备方法。
技术介绍
在化工领域中,苯、甲苯、二甲苯等化学物质统称为芳香烃。芳香烃作为一类常用的化工原料,应用十分广泛,市场需求巨大。在现有的芳香烃生产工艺中,通常都包括不饱和烯烃脱除工序,既利用脱烯烃催化剂脱除芳香烃半成品中含有的微量不饱和烯烃,如苯乙烯等,进而保证产品质量。现有的脱烯烃催化剂是颗粒状的白土,亦称颗粒白土。这种脱烯烃催化剂在使用过程中存在的主要问题是:催化活性较差,以致在使用过程中,消耗量较大,通常处理大约7200吨含有不饱和烯烃的芳香烃就需要使用1吨催化剂,从而加大了芳香烃的生产成本。
技术实现思路
本专利技术的目的是为人们提供一种脱烯烃催化剂的制备方法,以便使该催化剂具有良好的催化活性,进而解决现有技术存在的上述问题。本专利技术提供的脱烯烃催化剂是这样实现的,它包括:稀土金属氧化物颗粒,其特征在于该颗粒还载有活性物质,并使颗粒重量占两者总重量的90-99.9%。活性物质重量占两者总重量的0.1-10%。本专利技术提供的脱烯烃催化剂的制备方法是浸渍法。上述 ...
【技术保护点】
一种脱烯烃催化剂,包括稀土金属氧化物颗粒,其特征在于该颗粒还载有活性物质,并使颗粒重量占两者总重量的90‑99.9%。活性物质重量占两者总重量的0.1‑10%。
【技术特征摘要】
1.一种脱烯烃催化剂,包括稀土金属氧化物颗粒,其特征在于该颗粒还载有活性物质,并使颗粒重量占两者总重量的90-99.9%。活性物质重量占两者总重量的0.1-10%。2.权利要求1所述的脱烯烃催化剂的制备方法,其特征在于该方法是浸渍法。3.根据权利要求2所述的脱烯烃催化剂的制备方法,其特征在于所述浸渍法依次包括以下工艺步骤。A、浸渍:将颗粒状的稀土金属氧化物装入转动容器内,按该颗粒重量10-40%的比例,取浓度为0....