本实用新型专利技术公开了一种木炭机制棒机用合金推进器,包括尾部、螺杆部、中部及螺纹部,所述中部连接所述尾部及螺杆部,所述中部自靠近所述尾部一端到靠近所述螺杆部一端的直径逐渐增大,所述螺纹部螺纹环绕所述中部的外围。本实用新型专利技术较好的实现了其发明专利技术目的,其设计的合金推进器提高了生产效率,使用寿命可以达到2000-50000小时不需要修复,减少了修复成本。(*该技术在2022年保护过期,可自由使用*)

Alloy propeller

The utility model discloses an alloy propeller mechanism charcoal stick machine, including the tail, the screw thread part and the central part, the middle part is connected, the tail and the screw part, the central near the close to the end of the screw diameter increases the tail end of the screw thread around the Ministry, the periphery of the central. The utility model has the advantages that the utility model realizes the purpose of the invention, the alloy propeller designed by the utility model improves the production efficiency, the service life can reach 2000-50000 hours without repairing, and the repair cost is reduced.

【技术实现步骤摘要】

本技术涉及一种木炭机,尤其涉及一种木炭机制棒机用推进器。 
技术介绍
推进器是木炭机的关键部件之一,通常出现问题会影响整个机制木炭生产,现有技术中的推进器在正常使用情况下,约12小时候后,一般应取下修复,但有些原料质地不同,可能需要更短的时间就需要取下修复,修复时采用的焊条耐磨性及耐热性也可能影响到使用时间,传统推进器最长时间可使用72-108小时。传统推进器不耐高温、不耐挤压、不耐磨,磨损快使用寿命短,修复后也很难回到原始状态,提高修复频率势必提高生产成本。 
技术实现思路
本技术的目的是为木炭机制棒机提供一种新型的推进器;本技术是采用如下技术方案实现其专利技术目的的,合金推进器,包括尾部、螺杆部、中部及螺纹部,所述中部连接所述尾部及螺杆部,所述中部自靠近所述尾部一端到靠近所述螺杆部一端的直径逐渐增大,所述螺纹部螺纹环绕所述中部的外围。本技术为实现耐磨、耐高温、耐挤压,提高使用寿命的目的,在推进器螺纹部上镶上与螺纹部同样形状的合金片。由于采用了上述技术方案,本技术较好的实现了其专利技术目的,其设计的合金推进器提高了生产效率,使用寿命可以达到2000-50000小时不需要修复,减少了修复成本。 附图说明图1是本技术合金推进器的结构示意图; 具体实施方式下面结合附图对本技术作进一步描述。将合金片镶好焊接在推进器螺纹部上。 如图1所示,本技术合金推进器,所述的这种合金推进器包括包括尾部1、螺杆部3、中部2及螺纹部4,所述中部连接所述尾部及螺杆部,所述中部2自靠近所述尾部1一端到靠近所述螺杆部3一端的直径逐渐增大,所述螺纹部4螺纹环绕所述中部2的外围。推进器长508mm,在推进器尾部1端至200mm处镶上同轴心,同螺纹合金片。 本文档来自技高网...

【技术保护点】
合金推进器,其特征在于:在所述的推进器螺纹上镶上与螺纹同样形状的合金片。

【技术特征摘要】
1.合金推进器,其特征在于:在所述的推进器...