The invention provides an organic light emitting diode display panel. The organic light emitting diode display panel includes: a glass bottom plate; a first substrate, which is set on the glass bottom plate; a first high temperature resistant thermal conductive layer, which is set on the first substrate; a stress buffer layer, which is set on the first high temperature resistant thermal conductive layer; a second high temperature resistant thermal conductive layer, which is set on the stress buffer layer; and a second substrate, which is set on the stress buffer layer. On the second heat-resistant conductive layer.
【技术实现步骤摘要】
有机发光二极管显示面板及其制造方法
本专利技术涉及显示
,特别涉及一种有机发光二极管显示面板及其制造方法。
技术介绍
有机发光二极管(organiclightemittingdiode,OLED)显示装置具有轻薄、主动发光、响应速度快、可视角大、色域宽、亮度高和功耗低等众多优点,因此OLED显示装置近几年受到人们的关注。在OLED显示装置制造过程中,OLED显示面板需要在不同的机台之间运送。另外,在各个机台中,OLED显示面板需要被机台的抓取构件(picker)上的吸嘴吸附,以在各个机台中进行工艺步骤处理。请参考图1,图1显示机台200的抓取构件21上的吸嘴211在吸附现有的OLED显示面板100时的示意图。现有的OLED显示面板100包括玻璃底板11、聚酰亚胺(polyimide,PI)基板12、OLED器件层13、薄膜封装层14、触控面板15、偏光片16。当吸嘴211吸附OLED显示面板100时,吸嘴211对OLED器件层13所施加的吸附力量(如图1中箭头所示)会对OLED显示面板211的区域111造成缺陷,使得OLED显示面板100产生吸附Mura问题 ...
【技术保护点】
1.一种有机发光二极管显示面板,其特征在于,所述有机发光二极管显示面板包括:一玻璃底板;一第一基板,设置在所述玻璃底板上;一第一耐高温导热层,设置在所述第一基板上;一应力缓冲层,设置在所述第一耐高温导热层上;一第二耐高温导热层,设置在所述应力缓冲层上;及一第二基板,设置在所述第二耐高温导热层上。
【技术特征摘要】
1.一种有机发光二极管显示面板,其特征在于,所述有机发光二极管显示面板包括:一玻璃底板;一第一基板,设置在所述玻璃底板上;一第一耐高温导热层,设置在所述第一基板上;一应力缓冲层,设置在所述第一耐高温导热层上;一第二耐高温导热层,设置在所述应力缓冲层上;及一第二基板,设置在所述第二耐高温导热层上。2.根据权利要求1所述的有机发光二极管显示面板,其特征在于,所述有机发光二极管显示面板还包括:一有机发光二极管器件层,设置在所述第二基板上;一薄膜封装层,设置在所述有机发光二极管器件层上;一触控面板,设置在所述薄膜封装层上;及一偏光片,设置在所述触控面板上。3.根据权利要求1所述的有机发光二极管显示面板,其特征在于,所述第一基板与所述第二基板是柔性基板,所述柔性基板的材质为聚酰亚胺。4.根据权利要求1所述的有机发光二极管显示面板,其特征在于,所述应力缓冲层的材质为氧化石墨烯且具有约60%的压缩率,所述第一耐高温导热层及所述第二耐高温导热层的材质为氧化石墨烯。5.根据权利要求1所述的有机发光二极管显示面板,其特征在于,所述第一耐高温导热层及所述第二耐高温导热层承受至少500℃的制程温度,及所述第一耐高温导热层及所述第二耐高温导热层的厚度在介于10微米与30微米之间。6.根据权利要求1所述的有机发光二极管显示...
【专利技术属性】
技术研发人员:袁朝煜,
申请(专利权)人:武汉华星光电半导体显示技术有限公司,
类型:发明
国别省市:湖北,42