The invention discloses a method for improving isocyanate propyl triethoxysilane, which relates to the technical field of coupling agents. The method is as follows: polyethylene glycol is added into the crude isocyanate propyl triethoxysilane, then vacuum distillation is carried out, the initial fraction is cut off, and the middle fraction is the product of isocyanate propyl triethoxysilane; the amount of polyethylene glycol is 5 20% of the crude isocyanate propyl triethoxysilane. The main advantages of the method are that the yield of isocyanate propyl triethoxysilane is increased, the production cost is reduced, and the economic benefit is improved.
【技术实现步骤摘要】
一种提高异氰酸酯基丙基三乙氧基硅烷收率的方法
本专利技术涉及异氰酸酯基丙基三乙氧基硅烷精馏
,尤其是涉及一种,提高异氰酸酯基丙基三乙氧基硅烷收率的方法。
技术介绍
3-异氰酸酯基丙基三乙氧基硅烷,CASNO.:24801-88-5,分子量:247;,结构式:无色液体。3-异氰酸酯基丙基三乙氧基硅烷是一种新型有机硅硅烷偶联剂,异氰酸酯基能与羟基、氨基等活泼基团反应,用于有机材料中,能起到显著偶联作用,尤其对无机材料有着优异的附着力。如用于纤维素或环糊精上的羟基反应,将纤维素或环糊精固定在硅胶上制成手性固定相,用于手性化合物的分离。
技术实现思路
本专利技术要解决的技术问题是提供一种提高异氰酸酯基丙基三乙氧基硅烷收率的方法,本方法的主要优点在于提高了异氰酸酯基丙基三乙氧基硅烷的收率,得到了高含量的异氰酸酯基丙基三乙氧基硅烷成品,大大提高了高温精馏过程中异氰酸酯基丙基三乙氧基硅烷成品的收率,降低了生产成本,提高了经济效益。本专利技术解决上述技术问题采用的技术方案是:一种提高异氰酸酯基丙基三乙氧基硅烷收率的方法,其特征在于:在异氰酸酯基丙基三乙氧基硅烷粗品中加入聚乙二醇 ...
【技术保护点】
1.一种提高异氰酸酯基丙基三乙氧基硅烷收率的方法,其特征在于:该方法为:在异氰酸酯基丙基三乙氧基硅烷粗品中加入聚乙二醇,然后再进行减压精馏,得到异氰酸酯基丙基三乙氧基硅烷成品;聚乙二醇的加入量占异氰酸酯基丙基三乙氧基硅烷粗品中异氰酸酯基丙基三乙氧基硅烷质量的5‑20%。
【技术特征摘要】
1.一种提高异氰酸酯基丙基三乙氧基硅烷收率的方法,其特征在于:该方法为:在异氰酸酯基丙基三乙氧基硅烷粗品中加入聚乙二醇,然后再进行减压精馏,得到异氰酸酯基丙基三乙氧基硅烷成品;聚乙二醇的加入量占异氰酸酯基丙基三乙氧基硅烷粗品中异氰酸酯基丙基三乙氧基硅烷质量的5-20%。2.根据权利要求1所述的一种提高异氰酸酯基丙基三乙氧基硅烷收率的方法,其特征在于,所述聚乙二醇的加入量占异氰酸酯基丙基三乙氧基硅烷粗品中异氰酸酯基丙基三乙氧基硅烷质量的8%-12%。3.根据权利要求...