The invention relates to the technical field of wood board processing, in particular to a kind of ash scraping material for cedar solid wood core and its usage. The fir solid wood core shaving material consists of the following weight ratio material: 20 wood bran 40 copies, 200 glue 230 copies and 25 flour 7 flour; the optimization is also included: magnesium stearate 8 26, Qiang Jiaji cellulose sodium 2 10 copies, polyethylene glycol 200 10 10 26. The invention provides a spice solid wood core shaving material, which is used to repair the crevice of the core of the plate, to improve the evenness, to fill the gap rate and to reach the E0 level of the methanol release, and to solve the quality problems of the plate deformation and cracking caused by the gap in the traditional preparation process.
【技术实现步骤摘要】
一种香杉实木板芯刮灰料及使用方法
本专利技术涉及木板加工
,具体涉及一种香杉实木板芯刮灰料及使用方法。
技术介绍
融安县是全国林业大县,也是全国生态保护重点县,现有香杉总面积125万亩,香杉蓄积量达413万立方米,年可采伐香杉12万立方米。环保家具成为家具行业的新势力,能够较好地迎合现代人们追求环保、生态、健康的新需求和生活理念。因此,新型生态板将是当前行业的生力军,生态板变形率小,用胶量少等优势,加上整体实木芯体结构优势,将逐步淘汰密度板、颗粒板、刨花板、三聚氰氨板等在整体衣柜、橱柜行业及其他家具中广泛使用,在板材行业中占绝对主导地位。香杉实木生态板以融安优质香杉木为原料,富含纯天然高负氧离子,成品独具香杉醇天然香,香杉木不仅可抵抗一般的酸、碱、油脂及酒精等溶剂的磨蚀,亦可防虫蛀,防潮耐腐,长期生活在其环境中可提高人体免疫力,缓解疲劳、舒解压力等保健作用。因此香杉实木板在市场上销售不断增加。香杉实木生态板的制作过程需要将杉木原料切割成木条,然后将木条进行拼接成板芯,再经其他步骤制作而成。由于木条切割后再拼接,拼接过程中会存在缝隙,传统制备过程中是直 ...
【技术保护点】
一种香杉实木板芯刮灰料,其特征在于,包括以下重量份比的物料组成:木糠20‑40份、胶水200‑230份、面粉7‑25份。
【技术特征摘要】
1.一种香杉实木板芯刮灰料,其特征在于,包括以下重量份比的物料组成:木糠20-40份、胶水200-230份、面粉7-25份。2.根据权利要求1所述的一种香杉实木板芯刮灰料,其特征在于,还包括以下重量份比的物料组成:硬脂酸镁8-26份、羟甲基纤维素钠2-10份、聚乙二醇-20010-26份。3.根据权利要求2所述的一种香杉实木板芯刮灰料,其特征在于,包括以下重量份比的物料组成:木糠30份、胶水220份、面粉15份、硬脂酸镁17份、羟甲基纤维素钠6份和聚乙二醇-20017份。4.根据权利要求1或2所述的一种香杉实木板芯刮灰料,其特征在于,所述胶水选自大豆基木材胶黏剂、木质素木材胶黏剂、淀粉胶粘剂中的一种或几种。5.根据权利要求1或2所述的一种香杉实木板芯刮灰料,其特征在于,所述木糠的粒径为120-220μm。6.一种权利要求1所述香杉实木板芯刮灰料的使用方法,其特征在于,按重量份比,取各物料,包括以下步骤:S1.取面粉加水调节至含水量为25-40%,然后在35-50℃的条件下不断搅拌30-90min,然后通过孔径为0.1-...
【专利技术属性】
技术研发人员:唐胜荣,叶新忠,荣波,
申请(专利权)人:广西壮象木业有限公司,
类型:发明
国别省市:广西,45