一种固体自润滑衬套的制造方法技术

技术编号:17612815 阅读:14 留言:0更新日期:2018-04-04 04:48
本发明专利技术属于轴承制造领域,具体地说是一种自润滑轴承衬套的制造方法。加工工艺简便,涉及设备、工装少,产品成本低廉,主要技术特征是将粉末状固体自润滑材料装填在锥形压制模与衬套金属基体组成的环状缝隙中,衬套基体的工作基面先经粗化处理,再用压力机经压力被覆或嵌入,使衬套基体与固体润滑材料牢固结合,经烧结塑化,最后机械精加工成制品。

A method of manufacturing solid self lubricating bushing

The invention belongs to the field of bearing manufacturing, in particular a manufacturing method for a self - lubricating bearing bushing. The processing technology is simple, involving equipment, tooling, production cost is low, the main technical features are powdered solid self-lubricating materials filled in the tapered mold and bushing metal matrix composed of annular gap, the work surface by liner matrix roughening treatment, then the pressure by pressure covered or embedded in the matrix and the bushing solid lubricating material combined firmly by sintering plasticizing, finally finishing machinery into products.

【技术实现步骤摘要】
一种固体自润滑衬套的制造方法
本专利技术属于轴承制造领域,具体地说是一种自润滑滑动轴承衬套的制造方法。
技术介绍
镶嵌型固体自润滑轴承适用于在不能使用润滑油或使用润滑油极不方便的工况领域。
技术实现思路
本专利技术属于轴承制造领域,具体地说是一种自润滑轴承衬套的制造方法。具体实施方式1.将固体自润滑材料填装在锥形压制模与衬套基体组成的环状缝隙中,使用压力机推压衬套基体使自润滑粉末材料与衬套基体在工作基面上形成牢固结合。2.经烧结塑化,最后机械精加工成制品,衬套基体的工作基面在使用压力机前先经粗化处理,粗化处理的方法是采用烧结球形铜合金粉或机械加工。

【技术保护点】
将固体自润滑材料填装在锥形压制模与衬套基体组成的环状缝隙中,使用压力机推压衬套基体使自润滑粉末材料与衬套基体在工作基面上形成牢固结合。

【技术特征摘要】
1.将固体自润滑材料填装在锥形压制模与衬套基体组成的环状缝隙中,使用压力机推压衬套基体使自润滑粉末材料与衬套基体在工作基面上形成牢固结...

【专利技术属性】
技术研发人员:刘存福
申请(专利权)人:重庆向阳仪器有限公司
类型:发明
国别省市:重庆,50

网友询问留言 已有0条评论