The invention discloses a method for automatic control of sinter basicity, which comprises the following steps: when the line set when the alkalinity known, according to the Ca CaO content computing process model of batching time calculated to predict sinter CaO calculated that the correction coefficient J value; adoption; the numerical CaO of sinter; sinter obtained numerical SiO2; numerical calculate the midline of sinter CaO should be controlled; calculate midline CaO should draw ingredients model; prediction of sinter SiO2 calculated with Ca calculates the difference between central and divided by Ca calculation, the sinter basicity correction value; calculation of mixing model by changing the sinter basicity correction value, precision adjustment limestone, alkalinity adjustment. The purpose is to provide an automatic control method for sinter alkalinity, which can solve the problems of artificial adjustment in a timely manner, strong reliance on personal experience and unstable adjustment effect.
【技术实现步骤摘要】
烧结矿碱度自动控制方法
本专利技术属于铁矿粉烧结
,具体涉及一种烧结矿碱度自动控制的方法。
技术介绍
随着我国冶金行业的发展,高炉不断向大型化发展,大型化高炉对烧结矿质量的要求也越来越高。烧结矿碱度(行业一般用二元碱度来表示,即烧结矿的CaO含量和SiO2含量的比值)作为烧结矿质量评判的一个重要指标,其一级品率和合格率对高炉炉渣碱度的控制及操作影响很大,烧结矿碱度越稳定,高炉铁水质量越好。因此,烧结矿碱度稳定率的提升,对提高高炉铁水质量意义重大。传统的碱度控制思路是根据碱度实测值与碱度目标值的差值ΔR进行判断和调整:①一批|ΔR|≥0.05倍,以该批碱度值与目标值为依据进行计算,作“1/2”调整;②一批|ΔR|≥0.03倍,以该批碱度值与目标值为依据进行计算,作“1/3”调整;③连续三批|ΔR|≥0.02倍,以该三批的碱度平均值与目标值为依据进行计算,作“1/3”调整;④连续四批ΔR为正值或负值时,以该四批的碱度平均值与目标值为依据进行计算,作“1/3”或“1/4”调整。由于影响烧结矿碱度的因素较多,如受原料配比变化、成分波动、下料波动等因素影响,传统的检测 ...
【技术保护点】
一种烧结矿碱度自动控制方法,其特征在于,包括以下步骤:步骤S1:当已知设定的碱度中线时,根据配料模型计算的CaO含量Ca计算进行流程时间推算得出预测烧结矿CaO推算值;步骤S2:根据烧结矿检化验情况得到修正系数J,对修正系数J进行差值逻辑关系判定,得出修正系数J采纳值,用J采纳表示;步骤S3:用Ca计算乘以修正系数J采纳,得出实际能够生产出的烧结矿CaO数值,用Ca核算表示;步骤S4:追踪烧结矿SiO2数值,以10批求均值法作为追踪计算,得出用于碱度计算的烧结矿SiO2数值,用烧结矿SiO2推算表示;步骤S5:根据烧结矿SiO2推算和烧结矿碱度中线R中线,计算出烧结矿CaO ...
【技术特征摘要】
1.一种烧结矿碱度自动控制方法,其特征在于,包括以下步骤:步骤S1:当已知设定的碱度中线时,根据配料模型计算的CaO含量Ca计算进行流程时间推算得出预测烧结矿CaO推算值;步骤S2:根据烧结矿检化验情况得到修正系数J,对修正系数J进行差值逻辑关系判定,得出修正系数J采纳值,用J采纳表示;步骤S3:用Ca计算乘以修正系数J采纳,得出实际能够生产出的烧结矿CaO数值,用Ca核算表示;步骤S4:追踪烧结矿SiO2数值,以10批求均值法作为追踪计算,得出用于碱度计算的烧结矿SiO2数值,用烧结矿SiO2推算表示;步骤S5:根据烧结矿SiO2推算和烧结矿碱度中线R中线,计算出烧结矿CaO应该控制的中线数值,用Ca中线表示;步骤S6:根据Ca中线和配料模型计算CaO的对应关系,计算出配料模型计算应该得出的CaO中线,用Ca计算中线表示;步骤S7:用Ca计算中线和Ca计算之间的差值除以预测烧结矿SiO2推算,得出烧结矿碱度修正值,用R修正值...
【专利技术属性】
技术研发人员:安钢,王洪江,石江山,秦雪刚,刘莎莎,史凤奎,樊统云,康海军,裴元东,赵景军,王同宾,熊大林,杨伟强,周检平,张国超,程峥明,罗尧升,陈绍国,赵建峰,吴学亮,陈见见,贾慧敏,李佳,刘万里,