The invention discloses a cleaning method for forced circulation vacuum evaporation method phosphoric acid concentrating device, which comprises the following steps: (1) add washing water circulation loop composed to the evaporation chamber, heat exchanger and circulating pump; (2) concentrated sulfuric acid is added to the wash water circulation loop; (3) the washing liquid washing cleaning cycle in the circulation loop; (4) discharged from the washing liquid; its characteristic is: step (2) in concentrated sulphuric acid is added from the evaporation chamber. The sulfuric acid is directly added to the evaporation chamber, and the dilution heat can be quickly transmitted and lost, and local overheating can not occur, and the service life of the equipment can be prolonged.
【技术实现步骤摘要】
本方法用于湿法磷酸生产中的浓縮装置,具体地说是一种清洗磷酸浓 縮装置的方法。
技术介绍
用二水法生产的磷酸浓度一般为25 35%P205,随着高品位磷矿资 源的枯竭,目前大多数企业使用低品位磷矿生产磷酸,根据工艺要求,磷 酸生产浓度进一步减低。比如,申请人公司目前采用宜昌地区的低品位磷 矿,过滤磷酸浓度一般在22 25%P205。因此过滤磷酸必须加以浓縮。 目前磷酸浓縮流程一般采用强制循环真空蒸发流程、罗纳-普郎克磷酸浓 縮流程和斯温森磷酸浓縮流程。典型的强制循环真空蒸发系统主要包括循 环回路、除沫器、氟吸收设备、冷却器和真空系统。循环回路如图1所示, 由蒸发室3、热交换器1和循环泵6等组成,图中管道2通向除沫器。系 统经过一段时间的运行操作,热交换器的内壁产生盐类沉积和结垢,阻碍 热量传递。通常采用5%硫酸溶液对系统进行清洗除垢。其方法如下首 先向循环回路中加入洗涤水,待洗涤水达到一定量后,将98%的浓硫酸由 管道4通过蒸发室3与循环泵6之间的连通管5加入循环回路的洗涤水中, 控制加入量使洗涤液酸浓稀释到5%左右,然后开车使洗涤液在循环回路 中循环洗涤,直至清洗结束,再将洗涤液排出。由于浓硫酸加入洗涤水中 时会释放大量的稀释热,大量的热量短时间内难以散发出去,导致硫酸加 入点处的温度高达12(TC以上,由于温度偏高,硫酸加入点的连通管腐蚀速度很快,使用寿命较短。
技术实现思路
发了解决上述硫酸加入点温度高而导致的设备腐蚀快的问题,本专利技术 提供了一种强制循环真空蒸发法磷酸浓縮装置的清洗方法,通过改变加酸 位置,可以使硫酸稀释热有效地扩散开来,降低设备 ...
【技术保护点】
强制循环真空蒸发法磷酸浓缩装置的清洗方法,包括以下步骤:(1)、向由蒸发室[3]、热交换器[1]和循环泵[6]组成的循环回路中加入洗涤水;(2)、向循环回路的洗涤水中加入浓硫酸;(3)、使洗涤液在循环回路中循环清洗除垢;(4)排出洗涤液;其特征是:步骤(2)中的浓硫酸由蒸发室[3]加入。
【技术特征摘要】
1、强制循环真空蒸发法磷酸浓缩装置的清洗方法,包括以下步骤(1)、向由蒸发室[3]、热交换器[1]和循环泵[6]组成的循环回路中加入洗涤水;(2...
【专利技术属性】
技术研发人员:张福华,郭晓彬,何志民,许进冲,
申请(专利权)人:安徽六国化工股份有限公司,
类型:发明
国别省市:34[中国|安徽]