The invention discloses an environment-friendly PVC formula for low cost, the laying of pipelines, which is characterized in that made of the following raw materials in weight portion: two formic acid and two octyl phthalate 14 foaming agent 6 18 copies, 10 copies, 9 copies of 3 ACR modified, antistatic agent 12 17, nano calcium 7 12 copies, 8 copies of the 4 fossil wax chloride, titanium dioxide, 2 8, PE wax 0.5 3, six three 6 phosphoryl methyl amine 8, plasticizer 1 2 copies, 1.3 copies of 0.5 additives. The invention has the advantages of light weight, wear resistance, flame retardance, skid resistance, moisture resistance, etc., and is relatively low, and is suitable for popularization and application, and is relatively low, and is suitable for popularization and application.
【技术实现步骤摘要】
一种用于管道铺设的低成本、环保PVC配方
本专利技术涉及塑胶管道
,具体涉及一种用于管道铺设的低成本、环保PVC配方。
技术介绍
PVC管材的主要成分是聚氯乙烯,另外加入其它成分来增强其耐热性、韧性、延展性等。PVC在当今世界上深受喜爱,是颇为流行并广泛应用的一种合成材料。PVC管材是一种成熟的管材,主要应用于给排水工程。PVC管材具有耐酸、耐碱、耐腐蚀、强度高等优点,但抗冲性能比较差。
技术实现思路
本专利技术提供一种用于管道铺设的低成本、环保PVC配方,利用该配方制造出来的PVC管材可以增强抗冲性能及强度。为达到上述目的,本专利技术一种用于管道铺设的低成本、环保PVC配方,其特征在于由下列重量份的原料制成:邻苯二甲酸二辛酯14-18份,发泡剂6-10份,ACR改性3-9份,抗静电剂12-17份,纳米钙7-12份,氯化石蜡4-8份,钛白粉2-8份,PE蜡0.5-3份,六甲基磷酰三胺6-8份,增塑剂1-2份,助剂0.5-1.3份。作为优选,由下列最优配比原料制成:邻苯二甲酸二辛酯16份,发泡剂8份,ACR改性6份,抗静电剂13份,纳米钙8份,氯化石蜡5份,钛白粉 ...
【技术保护点】
一种用于管道铺设的低成本、环保PVC配方,其特征在于由下列重量份的原料制成:邻苯二甲酸二辛酯14‑18份,发泡剂6‑10份,ACR改性3‑9份,抗静电剂12‑17份,纳米钙7‑12份,氯化石蜡4‑8份,钛白粉2‑8份,PE蜡0.5‑3份,六甲基磷酰三胺6‑8份,增塑剂1‑2份,助剂0.5‑1.3份。
【技术特征摘要】
1.一种用于管道铺设的低成本、环保PVC配方,其特征在于由下列重量份的原料制成:邻苯二甲酸二辛酯14-18份,发泡剂6-10份,ACR改性3-9份,抗静电剂12-17份,纳米钙7-12份,氯化石蜡4-8份,钛白粉2-8份,PE蜡0.5-3份,六甲基磷酰三胺6-8份,增塑剂1-2份,助剂0.5-1.3份。2.如权利要求1所述的一种用于管道铺设的低成...
【专利技术属性】
技术研发人员:黄定荣,方爱珍,姜亚丽,
申请(专利权)人:东台市荣达塑业有限公司,