A new process for dyeing polyester / cotton knitted fabric, which comprises the following steps: pretreatment, one bath dyeing of polyester / cotton dyeing, acid neutralization, deoxidization and washing water, acid, TCW cleaning, hot washing and washing water, solid color, compared with the traditional process, the process uses a bath agent James TCB N will corsa pretreatment and dyeing process of polyester from merger, achieve oxygen one bath dyeing of polyester, polyester with no cleaning, while reducing heat washing times and two times reduction cleaning, direct dyeing, reduced by TCW technology; environmental protection cleaning technology of dyeing cotton, instead of the traditional 95 DEG C the two soaping process, while reducing heat washing times, environmental protection and low relative COD reduces the burden of sewage treatment, improve efficiency, reduce pollution emissions, to achieve the effect of energy saving and emission reduction.
【技术实现步骤摘要】
一种涤棉针织物的染色新工艺
本专利技术涉及一种染色工艺,具体涉及一种涤棉针织物的染色新工艺。
技术介绍
纺织品染整是我国的一个传统行业,也是纺织工业的一个重要环节,染整工业的水平很大程度上代表一个国家纺织工业的水平,它的发展起着十分重要的作用,众所周知,纺织物胚布基于本身纤维中棉籽、灰份杂质、油份等与纺造过程中产生的油污等成份,在后续染色工序前必须先去除这油份、杂质等成份,这就是前处理工序,经降解、乳化或溶解等物理化学方法处理后,提高织物布面光洁、上染率、增强均匀匀染性、减少染色次品率;在染整加工染色后处理工序则是将染色织物上沾附的布毛、浮色、杂质等,经过多次清洗、皂洗等工艺得到整洁的布面,确保产品各项牢度及其物理、外观指标达到要求。传统的加工方式一般先氧漂前处理,再进行分散/活性二浴二步法染色,即在弱酸性条件下染涤;再用保险粉加碱还原清洗,去除涤纶纤维表面以及沾污在棉组份上的分散染料;然后用醋酸中和,再以活性染料染棉组份;最后进行水洗并用皂洗剂进高温皂洗后处理,该工艺复杂,耗时、耗水、耗能,生产成本也较高,也排放出大量的废水,而在传统前处理和染色后处理工序上的水 ...
【技术保护点】
一种涤棉针织物的染色新工艺,其特征在于:包括以下步骤:第一步,前处理/染涤一浴:(1)、加水,升温至35‑45℃,加入雅可赛TCB‑N和染料,接着以1‑1.5℃/min升温至125‑135℃,保温25‑35min,然后以0.8‑1.5℃/min降至75‑85℃,加入液碱和双氧水,保温45‑55分钟,放水;(2)、加入45‑55℃的水,加入HAc,清洗5‑15min,放水;(3)、加入45‑55℃的水,加入除氧酶,除氧10‑20min,放水;第二步,染棉:加水,加入元明粉、染料,调节水溶液PH≦6.5,以0.5‑1.5℃/min升至45‑55℃,加入纯碱、固色碱,保温55‑6 ...
【技术特征摘要】
2017.01.20 CN 20171004815751.一种涤棉针织物的染色新工艺,其特征在于:包括以下步骤:第一步,前处理/染涤一浴:(1)、加水,升温至35-45℃,加入雅可赛TCB-N和染料,接着以1-1.5℃/min升温至125-135℃,保温25-35min,然后以0.8-1.5℃/min降至75-85℃,加入液碱和双氧水,保温45-55分钟,放水;(2)、加入45-55℃的水,加入HAc,清洗5-15min,放水;(3)、加入45-55℃的水,加入除氧酶,除氧10-20min,放水;第二步,染棉:加水,加入元明粉、染料,调节水溶液PH≦6.5,以0.5-1.5℃/min升至45-55℃,加入纯碱、固色碱,保温55-65min,接着再以0.8-1.5℃/min升至55-65℃,保温45-55min,放水,再清水洗涤;第三步,TCW清洗:(1)、加入45-55℃的水,加入HAc,清洗5-15min,放水;(2)、加水,再加入雅可赛TCW,以2-4℃/min升至85-95℃,保温10-20m...
【专利技术属性】
技术研发人员:张鑫,陈澄清,陈孝烨,吴华,潘立潮,
申请(专利权)人:福建凤竹纺织科技股份有限公司,
类型:发明