The invention discloses a layer by layer self-assembled thin film and a preparation method and application thereof. A layered self assembled film is formed by adding a polymer layer with opposite points and adding charged treatment drugs, and a negative pressure suction device is used to pump the liquid phase of the liquid to accelerate the time of the rearrangement of the polymer distribution. The design is applied to various wounds; the invention can form a thin film of 100 ~ 20000nm. The material in contact with the organism is significantly reduced and the rejection of the foreign body is reduced. The invention has wide range of material selection and drug selection. We can choose the kinds and dosage of drugs to achieve the effect of antibacterial, anti-inflammatory and wound healing. The multilayer self assembled film has flexible and convenient processability, adapts to the repair needs of many kinds of damaged wounds, and the quality of the product is stable and the reproducibility is good.
【技术实现步骤摘要】
一种层层自组装薄膜及其制备方法和应用
本专利技术属于组织工程领域,特别涉及一种层层自组装薄膜及其制备方法和应用。
技术介绍
层层自组装技术(layer-by-layerself-assembly,LbL)是依靠不同物质间的静电、氢键、化合键等作用力,把不同种类及功能的物质按照一定顺序组装成超薄膜的技术。它利用物质间的相互作用交替吸附在基底表面以构建纳米至微米级多层膜。由于是一层层进行组装,使得膜结构易于调控,尤其是薄膜厚度可以实现在纳米级别精细调控。传统的自组装技术需要固体材料作为基底,反复在不同材料溶液中浸润,在清水中清洗,形成自组装材料,过程耗时耗力。基于临床需求,尤其是与外界相通的组织器官治疗需求,急需专利技术一种省时省力的层层自组装方法来制作性质优良的创面敷料。皮肤,作为人体表面积最大的器官,是阻止微生物入侵,维持机体内环境稳定的坚固防线,具有重要的化学、物理和生物屏障功能。各种皮肤缺损性损伤,包括烧伤(热力、电或化学烧伤),糖尿病足,周围血管炎症、栓塞引起的皮肤溃疡,机械力引起的大片皮肤缺损等会引起皮肤屏障功能缺失,运用敷料覆盖创面,临时作为体表保护屏障 ...
【技术保护点】
一种层层自组装薄膜的制备方法,其特征在于包括如下步骤:1)将凝胶材料溶液铺展到基底上,将其凝固成固态;2)在铺有凝胶材料的基底上,铺加与凝胶材料所带电性相反的离子聚合物溶液,待其吸附于基底,吸去未反应溶液;再铺加与前述离子聚合物溶液电性相反的离子聚合物溶液,待其吸附于自组装层,吸去未反应溶液;3)循环操作步骤2)直至所需层数;4)在自组装层上滴加带电的治疗药物溶液,待吸附于自组装层后,吸去未反应溶液,再铺加与药物电性相反的离子聚合物溶液,待材料吸附于自组装层后,吸去未反应溶液;5)循环操作步骤4)至所需层数;6)将铺于基底的凝胶材料转为液态,直接于凝胶材料上取出自组装薄膜; ...
【技术特征摘要】
1.一种层层自组装薄膜的制备方法,其特征在于包括如下步骤:1)将凝胶材料溶液铺展到基底上,将其凝固成固态;2)在铺有凝胶材料的基底上,铺加与凝胶材料所带电性相反的离子聚合物溶液,待其吸附于基底,吸去未反应溶液;再铺加与前述离子聚合物溶液电性相反的离子聚合物溶液,待其吸附于自组装层,吸去未反应溶液;3)循环操作步骤2)直至所需层数;4)在自组装层上滴加带电的治疗药物溶液,待吸附于自组装层后,吸去未反应溶液,再铺加与药物电性相反的离子聚合物溶液,待材料吸附于自组装层后,吸去未反应溶液;5)循环操作步骤4)至所需层数;6)将铺于基底的凝胶材料转为液态,直接于凝胶材料上取出自组装薄膜;所述的离子聚合物溶液铺加方式为滴加、灌注或浸润,时间为20秒~3分钟,所述吸去未反应溶液的方式为负压吸引器抽吸。2.如权利要求1所述的层层自组装薄膜的制备方法,其特征在于所述的凝胶材料为明胶。3.如权利要求1所述的层层自组装薄膜的制备方法,其特征在...
还没有人留言评论。发表了对其他浏览者有用的留言会获得科技券。