Lithium ion capacitor, comprising: an anode, the anode comprises a conductive support, coated on a conductive support on the first mixture, comprising: from coconut shell carbon powder; conductive carbon black; PVDF adhesive, their quantity as defined in this paper; and the PVDF adhesive weight average molecular weight of 300000 to 400000 in the first second; coating mixture mixture, second mixture containing lithium metal particles of micron size, its encapsulation shell, the encapsulating shell including LiPF6, mineral oil and thermoplastic adhesive. Also disclosed are methods of making and using lithium ion capacitors.
【技术实现步骤摘要】
【国外来华专利技术】锂离子电容器中的聚偏二氟乙烯阳极粘合剂优先权申请的交叉参考本申请根据35U.S.C.§120,要求2015年1月30日提交的美国申请序列第14/610811号的优先权,本文以该申请为基础并将其全文通过引用结合于此。相关申请的交叉参考本申请涉及如下同时提交的且共同拥有和转让的USSN申请:2015年1月30日提交的题为“COKESOURCEDANODEFORLITHIUMIONCAPACITOR(用于锂离子电容器的源自焦炭的阳极)”的第14/610,752号;2015年1月30日提交的题为“ANODEFORLITHIUMIONCAPACITOR(用于锂离子电容器的阳极)”的第14/610782号;2015年1月30日提交的题为“PHENOLICRESINSOURCEDCARBONANODEINALITHIUMIONCAPACITOR(锂离子电容器中的源自酚醛树脂碳阳极)”的第14/610848号;以及2015年1月30日提交的题为“CATHODEFORLITHIUMIONCAPACITOR(用于锂离子电容器的阴极)”的第14/610868号,但是本文没有要求它们的优先 ...
【技术保护点】
一种锂离子电容器,其包括:阳极,其包含:导电支撑:涂覆在所述导电支撑上的第一混合物,其包含:源自椰壳粉的碳,它的量是85‑95重量%;导电炭黑,它的量是1‑8重量%;以及PVDF粘合剂,它的量是3‑10重量%,其中,重量%是基于所述第一混合物的总重计,以及其中,所述PVDF粘合剂的重均分子量是300,000至400,000;以及涂覆在所述第一混合物上的第二混合物,所述第二混合物包含微米尺寸锂金属颗粒,其具有包含LiPF6、矿物油和热塑性粘合剂的包封壳。
【技术特征摘要】
【国外来华专利技术】2015.01.30 US 14/610,8111.一种锂离子电容器,其包括:阳极,其包含:导电支撑:涂覆在所述导电支撑上的第一混合物,其包含:源自椰壳粉的碳,它的量是85-95重量%;导电炭黑,它的量是1-8重量%;以及PVDF粘合剂,它的量是3-10重量%,其中,重量%是基于所述第一混合物的总重计,以及其中,所述PVDF粘合剂的重均分子量是300,000至400,000;以及涂覆在所述第一混合物上的第二混合物,所述第二混合物包含微米尺寸锂金属颗粒,其具有包含LiPF6、矿物油和热塑性粘合剂的包封壳。2.如权利要求1所述的电容器,其特征在于,所述导电支撑是铜箔或铝箔。3.如权利要求1-2中任一项所述的电容器,所述电容器还包括:分隔器;与所述分隔器相连的阴极电极,所述阴极电极包括:源自小麦粉的碱活化碳,它的量是80-95重量%;氟化聚合物,它的量是3-12重量%;和炭黑,它的量是1-8重量%;以及电解质,其包含非水性且质子惰性溶剂中...
【专利技术属性】
技术研发人员:K·P·加德卡埃,R·S·卡达姆,
申请(专利权)人:康宁股份有限公司,
类型:发明
国别省市:美国,US
还没有人留言评论。发表了对其他浏览者有用的留言会获得科技券。