一种自溢胶粘结式疏绕线盘制造技术

技术编号:15866539 阅读:134 留言:0更新日期:2017-07-23 15:39
本实用新型专利技术公开了一种自溢胶粘结式疏绕线盘,它包括支架(1),支架(1)上设有多组绕线筋(2);绕线筋(2)之间设有绕线槽(3),绕线槽(3)内绕制有绕线组(4);所述绕线组(4)包括线芯(7),线芯(7)外表面设有绝缘基膜(8),绝缘基膜(8)的内、外表面上设有粘合层(9)。本实用新型专利技术不仅能够在生产过程中降低废品率,还具有生产成本低、外观精良和安全系数高的优点。

Self overflow adhesive wrapped winding reel

The utility model discloses a self adhesive type winding disk overflow dredging, which comprises a support bracket (1), (1) is provided with a plurality of winding bars (2); winding rib (2) winding groove is arranged between the winding groove (3), (3) in the wound around group (4); the winding (4). The line core (7), the wire core (7) are arranged on the external surface of the insulation substrate (8), (8) the base insulating film is arranged on the inner surface and the outer surface of the adhesive layer (9). The utility model not only can reduce the reject rate in the production process, but also has the advantages of low production cost, good appearance and high safety factor.

【技术实现步骤摘要】
一种自溢胶粘结式疏绕线盘
本技术涉及一种电磁炉用的疏绕线盘,特别是一种自溢胶粘结式疏绕线盘。
技术介绍
现有电磁炉线盘的绕线组绕制在支架上,为防止绕线组脱离掉落出支架,一般采用热压的方式实现绕线组的强制固定;主要是采用具有高温的钢模具将绕线组压制在支架上的绕线筋位上,使绕线筋的上端面强制受热变形挤压,把支架塑胶挤压到绕线槽的上部,将绕线槽的上部与绕线组固定。但是热压固定的方式容易导致支架压裂报废,钢模具上的温度以及热压变形的深度难以控制,容易导致支架热压变形的深度不一致,产生废品率较高,生产成本高;且线盘外观容易受热压不良的影响,热压过浅则支架上绕线筋受热变形较小,绕线组容易脱离支架;热压过深则支架上绕线筋受热变形太大,支架容易被压裂。热压固定的方式还容易导致绕线组被钢模具烫伤,导致绕线组露白破损出现线盘匝间短路,安全性较差等。因此,现有的电磁炉线盘在加工过程中产生的废品率较高,生产成本较高,线盘外观偏差较大,安全系数较低。
技术实现思路
本技术的目的在于,提供一种自溢胶粘结式疏绕线盘。本技术不仅能够在生产过程中降低废品率,还具有生产成本低、外观精良和安全系数高的优点。本技术的技术方案:一种本文档来自技高网...
一种自溢胶粘结式疏绕线盘

【技术保护点】
一种自溢胶粘结式疏绕线盘,其特征在于:包括支架(1),支架(1)上设有多组绕线筋(2);绕线筋(2)之间设有绕线槽(3),绕线槽(3)内绕制有绕线组(4);所述绕线组(4)包括线芯(7),线芯(7)外表面设有绝缘基膜(8),绝缘基膜(8)的内、外表面上设有粘合层(9)。

【技术特征摘要】
1.一种自溢胶粘结式疏绕线盘,其特征在于:包括支架(1),支架(1)上设有多组绕线筋(2);绕线筋(2)之间设有绕线槽(3),绕线槽(3)内绕制有绕线组(4);所述绕线组(4)包括线芯(7),线芯(7)外表面设有绝缘基膜(8),绝缘基膜(8)的内、外表面上设有粘合层(9)。2.根据权利要求1所述的一种自溢胶粘结式疏绕线盘,其特征在于:所述支架(1)底部设有多组...

【专利技术属性】
技术研发人员:高新忠孙亮邓杰洪城军
申请(专利权)人:杭州信多达电器有限公司
类型:新型
国别省市:浙江,33