一种涂料用催干剂制造技术

技术编号:15835983 阅读:44 留言:0更新日期:2017-07-18 14:39
本发明专利技术涉及涂料技术领域,尤其涉及一种涂料用催干剂。该一种涂料用催干剂以质量份计:异辛酸50-70份、五氧化二钒10-15份、芳烃溶剂油20-30份、稀土化合物10-15份、碳酸盐10-15份、镍化合物10-15份。本发明专利技术提供的一种涂料用催干剂,可用于芳烃溶剂及脂肪烃溶剂,可代替传统的钴、锰、铅、锌、钙混合金属在涂料工业中做催干剂的应用,可一次性加入涂料中,用料仅是传统催干剂的10%,具有用量少,经济效益明显,使用方便,便于管理的特点。

Drier for coating

The invention relates to the technical field of coatings, in particular to a drier for coating. The drying agent for this coating uses mass fraction: 50-70 octanoic acid, five oxide two vanadium, 20-30 aromatic hydrocarbon solvent oil, 10-15 rare earth compounds, 10-15 carbonate, 10-15 nickel compounds, 10-15 copies. Driers for coating provided by the invention can be used for aromatic solvents and aliphatic hydrocarbon solvent, can replace the traditional cobalt, manganese, lead, zinc and calcium in mixed metal drying agent application in the paint industry, can join in the paint material is only traditional driers with 10%. Less useful, obvious economic benefits, convenient use, convenient management features.

【技术实现步骤摘要】
一种涂料用催干剂
本专利技术涉及涂料
,尤其涉及一种涂料用催干剂。
技术介绍
催干剂是涂料不可缺少的助剂之一。传统的钴、铅、锰、锌、钙等催干剂,在使用时需按照不同比例调配,手续繁杂且添加量大,涂料生产企业急需一款能单独使用且用量较小的催干剂以降低人力物力成本。另外,钴、铅是有毒致癌物,当前涂料工业对于环保健康的要求越来越高,无毒催干剂无疑是发展趋势。
技术实现思路
针对现有技术的上述缺陷,本专利技术提供的一种涂料用催干剂,解决了传统的钴、铅、锰、锌、钙等催干剂,在使用时需按照不同比例调配,手续繁杂且添加量大,催化剂采用钴、铅为原料有毒致癌物的问题。为了达到上述目的,本专利技术提供如下技术方案:一种涂料用催干剂以质量份计:异辛酸50-70份、五氧化二钒10-15份、芳烃溶剂油20-30份、稀土化合物10-15份、碳酸盐10-15份、镍化合物10-15份。其中,所述异辛酸53份、五氧化二钒12份、芳烃溶剂油23份、稀土化合物12份、碳酸盐13份、镍化合物12份。其中,所述异辛酸65份、五氧化二钒14份、芳烃溶剂油27份、稀土化合物14份、碳酸盐15份、镍化合物15份。本专利技术的有益效本文档来自技高网...

【技术保护点】
一种涂料用催干剂,其特征在于,以质量份计:异辛酸50‑70份、五氧化二钒10‑15份、芳烃溶剂油20‑30份、稀土化合物10‑15份、碳酸盐10‑15份、镍化合物10‑15份。

【技术特征摘要】
1.一种涂料用催干剂,其特征在于,以质量份计:异辛酸50-70份、五氧化二钒10-15份、芳烃溶剂油20-30份、稀土化合物10-15份、碳酸盐10-15份、镍化合物10-15份。2.根据权利要求1所述的一种涂料用催干剂,其特征在于,所述异辛酸5...

【专利技术属性】
技术研发人员:孙学儒
申请(专利权)人:沈阳澳宇化工有限公司
类型:发明
国别省市:辽宁,21