The invention discloses a kind of activated carbon in the flask, including the inner bottle body, wherein the bottle body inner layer coated activated carbon layer, wherein the inner bottle body outer coating ceramic layer. The invention of activated carbon can absorb impurities in the liquid, remove the odor, and when aged wine can reduce the time Shen brewing wine, according to the experimental test can reduce Shen brewing time by 25%, through the activated carbon precipitation in the wine bottle liner better taste; the cost of activated carbon production in flask is low, through a special process improve the production efficiency.
【技术实现步骤摘要】
本专利技术涉及一种活性炭内胆瓶,属于内胆瓶的
技术介绍
现在市面上普通的瓶一般都是陶瓶、瓷瓶、玻璃瓶等,其用料单一,对盛装的液体没用什么特殊的功用。而且内胆瓶内部经常结垢,影响盛装的溶液质量。
技术实现思路
本专利技术目的是针对现有技术存在的缺陷提供一种活性炭内胆瓶。本专利技术为实现上述目的,采用如下技术方案:本专利技术一种活性炭内胆瓶,包括内胆瓶本体,其特征在于所述内胆瓶本体内层涂布活性炭层,所述内胆瓶本体外层涂布陶瓷层。所述内胆瓶本体内层涂布活性炭层。所述活性炭层的厚度为0.2-8mm或者大于8_。本专利技术具有如下优点:I)活性炭可以吸收液体中的杂质,去除异味,并且在陈放酒的时候可以减少酒的沉酿时间,根据实验检验可以减少25%的沉酿时间,通过活性炭内胆瓶沉酿的酒在口感上更佳;2)活性炭内胆瓶外形美观,因为通过特殊的烧制方法烧制出的瓶子在色泽上更加润泽;3)活性炭内胆瓶的制作成本低,通过专用工艺更加提高生产效率。附图说明图1:本专利技术结构示意图。具体实施例方式如图1所示,本专利技术一种活性炭内胆瓶,包括内胆瓶本体,所述内胆瓶本体内层涂布活性炭层1,所述内胆瓶本体外层涂布陶瓷层2。所述内胆瓶本体内层涂布多层活性炭层I。本专利技术优选活性炭层I的厚度为0.2_8mm。以上所述仅为本专利技术的优选实施例而已,并不用于限制本专利技术,尽管参照前述实施例对本专利技术进行了详细的说明,对于本领域的技术人员来说,其依然可以对前述各实施例所记载的技术方案进行修改,或者对其中部分技术特征进行等同替换。凡在本专利技术的精神和原则之内,所作的任何修改、等同替换、改 ...
【技术保护点】
一种活性炭内胆瓶,包括内胆瓶本体,其特征在于所述内胆瓶本体内层涂布活性炭层(1),所述内胆瓶本体外层涂布陶瓷层(2)。
【技术特征摘要】
还没有人留言评论。发表了对其他浏览者有用的留言会获得科技券。