The utility model discloses a test device for evaluating high temperature corrosion performance of oil pipe in low water cut and high production gas well, which belongs to the field of oil pipe corrosion evaluation. It includes the humidity regulating autoclave, the test autoclave and the waste waste liquid treatment system which are connected through the pipeline, and there is a one-way valve on the main pipe connected by the humidity regulating autoclave to the test autoclave, and the air supply system which is connected by the pipe and the humidity regulating autoclave and the test autoclave respectively, and the humidity is adjusted high pressure. There are heating devices in the kettle and the test autoclave, and the test solution is filled in the humidity regulating autoclave, and the test high pressure tank is equipped with a multistage electric agitator. The test sample is loaded in the test autoclave, and the pressure, humidity, pH value and temperature are also installed on the humidity regulating autoclave and the test autoclave. The test device. The design of the device is reasonable, and it can adjust and monitor many parameters in one test, satisfying the test requirements under multiple conditions.
【技术实现步骤摘要】
一种评价低含水率高产气井油管高温腐蚀性能的试验装置
本技术属于油井管腐蚀评价领域,具体涉及一种评价低含水率高产气井油管高温腐蚀性能的试验装置。
技术介绍
在油气田开采开发过程中,腐蚀是自始至终存在的严重问题。其中,在高产气井开采过程中,井筒中的高速流体对油管柱的高温腐蚀和冲蚀作用尤为显著。因为高速流体使腐蚀介质(H2S、CO2、Cl-、凝析水等)等在金属表面上运动,在机械磨损与腐蚀共同作用下,使腐蚀加速。例如,四川气田某些高产气井,日产气量可达100万方,日产水量约8万方,H2S、CO2等腐蚀性介质的含量高达150g/m3,对油管柱将产生严重腐蚀。为此,科技人员对油井管柱的高温腐蚀和冲蚀损伤机理、防护技术和预防措施等进行了大量的研究,同时也开发了一些研究油井管柱高温腐蚀和冲蚀腐蚀性能的试验装置。目前用于评价油井管柱高温腐蚀性能和冲蚀性能的常用设备为高温高压反应釜。常规配置的CORTEST动态高温高压釜最大操作温度可达350℃,最大操作压力可达35MPa。专门用于超临界腐蚀研究的高温高压釜最大操作温度可达600℃。更高压力等级的高温高压釜最大操作压力可达69MPa,103MPa,甚至138MPa。但是,常规高温高压反应釜存在以下不足:(1)受动力因素限制,一般只能模拟最高流速为5m/s的冲蚀环境;(2)一定温度下气液两相环境中不能调节腐蚀环境的湿度,无法模拟极低含水率高产气井的高温腐蚀和冲蚀环境。例如,当试验温度高于100℃,未达到临界压力时,模拟地层水已达到沸腾,甚至超临界状态,腐蚀试验结果与现场腐蚀情况相差太大。为此,科技人员研发了新型的模拟油井管柱高温 ...
【技术保护点】
1.一种评价低含水率高产气井油管高温腐蚀性能的试验装置,其特征在于,包括通过管路依次相连的湿度调节高压釜(25)、试验高压釜及废气废液处理系统(28),在湿度调节高压釜(25)与试验高压釜相连的主管道(26)上设有单向阀(16);还包括分别通过管路与湿度调节高压釜(25)和试验高压釜相连的供气系统(15);在湿度调节高压釜(25)和试验高压釜内均设有加热装置,湿度调节高压釜(25)内填充有试验溶液(19),试验高压釜中设有多级电动搅拌器(3),测试样品(33)承装于试验高压釜中;在湿度调节高压釜(25)和试验高压釜上还均设有用于实时监测试验压力、湿度、pH值和温度的测试装置。
【技术特征摘要】
1.一种评价低含水率高产气井油管高温腐蚀性能的试验装置,其特征在于,包括通过管路依次相连的湿度调节高压釜(25)、试验高压釜及废气废液处理系统(28),在湿度调节高压釜(25)与试验高压釜相连的主管道(26)上设有单向阀(16);还包括分别通过管路与湿度调节高压釜(25)和试验高压釜相连的供气系统(15);在湿度调节高压釜(25)和试验高压釜内均设有加热装置,湿度调节高压釜(25)内填充有试验溶液(19),试验高压釜中设有多级电动搅拌器(3),测试样品(33)承装于试验高压釜中;在湿度调节高压釜(25)和试验高压釜上还均设有用于实时监测试验压力、湿度、pH值和温度的测试装置。2.根据权利要求1所述的评价低含水率高产气井油管高温腐蚀性能的试验装置,其特征在于,加热装置包括主加热器(1)和副加热器(2),在湿度调节高压釜(25)底部设有主加热器(1);在试验高压釜的底部设有主加热器(1),周向侧壁内设有副加热器(2)。3.根据权利要求1所述的评价低含水率高产气井油管高温腐蚀性能的试验装置,其特征在于,在试验高压釜上设有第一温度计(5)、第一压力计(6)、第一pH计(7)及第一湿度计(14);在湿度调节高压釜(25)上设有第二温度计(22)、第二压力计(20)、第二pH计(18)及第二湿度计(21)。4.根据权利要求1所述的评价低含水率高产气井油管高温腐蚀性能的试验装置,其特征在于,供气系统(15)通过第一进气管(24)与湿度调节高压釜(25)相连,第一进气管(24)上设有第一进气阀(17),在湿度调节高压釜(25)顶部设有第一排气管(27),第一排气管(27)上设有第一排气阀(23);供气系统(15)通过第二进气管(8)与试验高压釜相连,第二进气管(8)上设有第二进气阀(12),试验高压釜与废气废液处理系统(28)通过第二排气管(...