The plastic ring for metallizing film of capacitor is divided into plastic ring, and the plastic ring is made of at least two thin plastic traps with interference fit. The utility model is changed from original molding to two forming or more than three times forming, that is, two rings combination or three or more ring combinations. The thin plastic ring is easy to cool in the forming process, the cooling process is not easy to deform, the plastic ring surface is smooth and smooth, the thickness of the plastic ring after the set is more than 6mm, to meet the strength demand.
【技术实现步骤摘要】
电容器用金属化薄膜分切用的塑料圈
本技术涉及一种电容器用金属化薄膜分切用的塑料圈。
技术介绍
生产电容器用的金属化薄膜,需按要求分切成14mm或19mm等不同宽度的条状,并将其缠绕在相同宽度的塑料圈上,形成一盘一盘的金属化薄膜。若干个相同宽度的金属化薄膜用塑料圈并排组成600mm宽的阵列,投入金属化膜分切自动化生产线。此时,对同种宽度的塑料圈的精度一致性要求高,即要求塑料圈与金属化薄膜的接触面需平整光滑,无凹陷、无凸起。由于塑料圈强度的需求,塑料圈的厚度要大于6mm,才能达到强度要求。而厚度大于6mm的塑料圈在一次成型后需要进行较长时间的冷却,冷却过程中较厚的厚度会造成塑料圈表面因缩水而下凹不平整。
技术实现思路
本技术的目的,是要提供一种电容器用金属化薄膜分切用的塑料圈,它表面光滑平整,无凹陷、无凸起,而且塑料圈的厚度大于6mm,塑料圈的强度符合生产要求。本技术是这样实现的,所述电容器用金属化薄膜分切用的塑料圈,它包括塑料圈,所述的塑料圈由至少两个过盈配合的薄形塑料圈套设而成。本技术的有益效果是,它由原来的一次成型,改为两次成型或三次以上成型,即两个套圈组合或三个以上套圈组合。较薄的塑料圈在成型过程容易冷却,冷却过程不易变形,塑料圈表面光滑平整,套设后的塑料圈厚度大于6mm,满足强度需求。附图说明图1为本技术立体示意图。图2为本技术的剖面示意图。图中:1.外圈,2.内圈,3.总厚度,4.宽度。具体实施方式本技术所述电容器用金属化薄膜分切用的塑料圈,如图1、2所示,它包括塑料圈,所述的塑料圈由两个过盈配合的薄形塑料圈套设而成。所述塑料圈包括外圈1和内圈2,内外圈的 ...
【技术保护点】
电容器用金属化薄膜分切用的塑料圈,它包括塑料圈,其特征是:所述的塑料圈由至少两个过盈配合的塑料圈套设而成。
【技术特征摘要】
1.电容器用金属化薄膜分切用的塑料圈,它包括塑料圈,其...