The invention discloses a building with concrete and preparation of construction method, which relates to the technical field of construction; it comprises the following components in parts by weight: 2 sand 3, 5, 4 phosphorus slag fly ash cement, 3 4 1 2 copies, 1 copies, 0.5 feed water alkali activator 0.2 0.5 copies, 0.2 copies, 0.1 gas agent filler 0.5 1 copies, 1.2 copies, 0.3 adhesive glue 1 Building 2; it follows the method: according to the weight and get good; the sand, phosphorus slag, fly ash, cement, water, filler material mixing and by mechanical mixer and, the stirring time is 10 15 minutes; then add alkali activator stir 3 5 minutes; the invention can achieve the required strength, and low preparation cost, and can realize the preparation, and the preparation time is short, high efficiency.
【技术实现步骤摘要】
一种建筑用混凝土及其制备施工方法
本专利技术涉及一种建筑用混凝土及其制备施工方法,属于建筑
技术介绍
从广义上来说,建筑学是研究建筑及其环境的学科。建筑学是一门横跨工程技术和人文艺术的学科。建筑学所涉及的建筑艺术和建筑技术、以及作为实用艺术的建筑艺术所包括的美学的一面和实用的一面,它们虽有明确的不同但又密切联系,并且其分量随具体情况和建筑物的不同而大不相同。现有的混凝土的各种组分通过一定的工艺加工制得,其未能达到所需要的强度,而且制备成本高,且不能实现现场制备,导致时间长。
技术实现思路
针对上述问题,本专利技术要解决的技术问题是提供一种建筑用混凝土及其制备施工方法。本专利技术的一种建筑用混凝土,它包括如下重量份数的组分:砂石2-3份、磷渣4-5份、粉煤灰3-4份、水泥1-2份、水料0.5-1份、碱类激发剂0.2-0.5份、发气剂0.1-0.2份、填充剂0.5-1份、粘合剂0.3-1.2份、建筑胶水1-2份。一种建筑用混凝土的制备施工方法,它的方法如下:步骤一、将重量份数的组分:砂石2-3份、磷渣4-5份、粉煤灰3-4份、水泥1-2份、水料0.5-1份、碱类 ...
【技术保护点】
一种建筑用混凝土,其特征在于:它包括如下重量份数的组分:砂石2‑3份、磷渣4‑5份、粉煤灰3‑4 份、水泥1‑2份、水料0.5‑1 份、碱类激发剂0.2‑0.5 份、发气剂0.1‑0.2份、填充剂0.5‑1份、粘合剂0.3‑1.2份、建筑胶水1‑2份。
【技术特征摘要】
1.一种建筑用混凝土,其特征在于:它包括如下重量份数的组分:砂石2-3份、磷渣4-5份、粉煤灰3-4份、水泥1-2份、水料0.5-1份、碱类激发剂0.2-0.5份、发气剂0.1-0.2份、填充剂0.5-1份、粘合剂0.3-1.2份、建筑胶水1-2份。2.一种建筑用混凝土的制备施工方法,其特征在于:它的方法如下:步骤一、将重量份数的组分:砂石2-3份、磷渣4-5份、粉煤灰3-4份、水泥1-2份、水料0.5-1份、碱类激发剂0.2-0.5份、发气剂0.1-0.2份、填充...