The invention discloses a steel plastic composite pressure pipe coextrusion composite bonding apparatus, including hole connecting joint, a telescopic rod and a sealing rubber capsule; the connector is connected to the left hole extruding along which the air pressure air outlet, the joint hole is arranged at the right end of powder outlet, and the right end connected to the fixed joint telescopic rod connecting hole; the sealing rubber sealing bag is fixed on the connecting rod, and the telescopic rod is fixed at the right end of the connecting rod is connected to a sealing bag. The steel plastic composite pressure pipe coextrusion adhesive composite stabilizer after use, shorten the sealing rubber capsule and coextrusion head distance, solve the long distance pipe and wire rope in the running process of sealing sponge and wall friction size caused by wire rope support hours is not enough the gap.
【技术实现步骤摘要】
一种钢塑复合压力管共挤粘接复合稳压装置
本专利技术涉及钢塑复合压力管生产设备
,具体是一种钢塑复合压力管共挤粘接复合稳压装置。
技术介绍
钢塑复合压力管是一种内外均有塑层,中间为氩弧对接焊钢管,钢管和塑层之间由专用胶粘剂进行粘接的五层复合管材。大口径钢塑复合压力管一般采用内塑层和粘接剂共挤通过空压风带压吹胀涂覆到钢管内表面的生产工艺方法。采用此工艺方法生产时,传统的海绵堵头密封通过钢丝绳连接,并在外塑层的冷却水处冷却,这样设计会造成一下工艺不稳定性:1、支撑牵引海绵的钢丝绳距离过长,管材在运行过程中密封海绵与管壁长时间摩擦海绵尺寸变小,造成钢丝绳支撑不够而下垂,钢丝绳下垂时与高温的塑料内管壁接触,容易在未冷却的部位产生起沟现象,导致管材报废;2、由于海绵密封处冷却位置距离共挤机头较远,管材共挤方式下靠空压风吹胀成型,当海绵与管壁摩擦而尺寸缩减时,将影响海绵处的风压密封性,引起空压风压力不稳的问题,空压风的压力不稳定,将造成内壁贴合不严、刚塑粘接不良,引起管材分层现象。
技术实现思路
本专利技术的目的在于提供一种钢塑复合压力管共挤粘接复合稳压装置,以解决上述背景技 ...
【技术保护点】
一种钢塑复合压力管共挤粘接复合稳压装置,其特征在于,包括气孔连接接头(1)、伸缩杆(3)和密封橡胶囊(5);所述气孔连接接头(1)左端连接至挤出机共挤流道上的空压风出口,气孔连接接头(1)右端设置有散风口(2),且气孔连接接头(1)右端固定连接至伸缩杆(3);所述密封橡胶囊(5)固定安装在密封囊连接杆(8)上,且伸缩杆(3)的右端固定连接至密封囊连接杆(8)。
【技术特征摘要】
1.一种钢塑复合压力管共挤粘接复合稳压装置,其特征在于,包括气孔连接接头(1)、伸缩杆(3)和密封橡胶囊(5);所述气孔连接接头(1)左端连接至挤出机共挤流道上的空压风出口,气孔连接接头(1)右端设置有散风口(2),且气孔连接接头(1)右端固定连接至伸缩杆(3);所述密封橡胶囊(5)固定安装在密封囊连接杆(8)上,且伸缩杆(3)的右端固定连接至密封囊连接杆(8)。2.根据权利要求1所述的钢塑复合压力管共挤粘接复合稳...