The embodiment of the invention discloses an activated carbon coating and a preparation method thereof, relating to the field of coating preparation. Raw materials for activated carbon coating of the invention comprises the following parts by weight: powdered activated carbon prepared 50 80 copies, 40 copies of 20 resin mixture, nano titanium dioxide 1 20 copies, 20 copies of 10 adhesive. The invention has the advantages of good coating selectivity, large adsorption capacity, fast adsorption speed, good abrasion resistance, corrosion resistance and good bacteriostatic effect, and is suitable for water, water pipes, kitchen and toilet articles, household products, etc. the utility model is an ideal odor eliminating product.
【技术实现步骤摘要】
一种活性炭涂层及其制备方法
本专利技术涉及一种活性炭涂层及其制备方法,属于涂层制备领域。
技术介绍
现代城镇居民长时间在室内渡过,各种新型材料、建筑添加剂以及装饰装修造成的室内空气的污染。除此之外,下水管道内异味重,细菌滋生,对人体有害。现有空气净化产品,效果差,持续时间短,吸收范围比较有限,针对性差。活性炭有很强的物理吸附和化学吸附功能,对气体、溶液中的无机或有机物质及胶体颗粒等都有良好的吸附能力,是一种性能优良的吸附剂。活性炭材料的化学性质稳定,机械强度高,耐酸、耐碱、耐热,不溶于水与有机溶剂,可以再生使用,已经广泛地应用于化工、环保、食品加工、冶金、药物精制、军事化学防护等各个领域。目前,活性炭材料被广泛用于污水处理、大气污染防治等领域,在治理环境污染方面越来越显示出其诱人的美好前景。
技术实现思路
本专利技术的实施例提供一种活性炭涂层及其制备方法,所制备得的涂层选择性好,吸附量大,吸附速度快,并且耐磨防腐,抑菌效果好,适用于下水水管道,厨卫用品,家居产品等,是理想的异味消除产品。为达到上述目的,本专利技术的实施例采用如下技术方案:一种活性炭涂层,由下列重量份的原料制成:粉状活性炭50-80份,树脂混合物20-40份,纳米二氧化钛1-20份,粘合剂10-20份。进一步的,所述树脂混合物是聚丙烯,聚四氟乙烯,环氧树脂的混合物。进一步的,所述树脂混合物是由下列重量份的原料制成:聚丙烯20-50份,聚四氟乙烯60-80份,环氧树脂20-50份。进一步的,所述树脂混合物是由下列重量份的原料制成:聚丙烯20-40份,聚四氟乙烯50-70份,环氧树脂30-40份。进 ...
【技术保护点】
一种活性炭涂层,其特征在于,由下列重量份的原料制成:粉状活性炭50‑80份,树脂混合物20‑40份,纳米二氧化钛1‑20份,粘合剂10‑20份。
【技术特征摘要】
1.一种活性炭涂层,其特征在于,由下列重量份的原料制成:粉状活性炭50-80份,树脂混合物20-40份,纳米二氧化钛1-20份,粘合剂10-20份。2.根据权利要求1所述的一种活性炭涂层,其特征在于,由下列重量份的原料制成:粉状活性炭60-75份,树脂混合物20-30份,纳米二氧化钛5-15份,粘合剂10-15份。3.根据权利要求2所述的一种活性炭涂层,其特征在于,所述树脂混合物是聚丙烯,聚四氟乙烯,环氧树脂的混合物。4.根据权利要求3所述的一种活性炭涂层,其特征在于,由下列重量份的原料制成:聚丙烯20-50份,聚四氟乙烯60-80份,环氧树脂20-50份。5.根据权利要求3所述的一种活性炭涂层,其特征在于,由下列重量份的原料制成:聚丙烯20-40份,聚四氟乙烯50-70份,环氧树脂30-40份。6.根据权利要求2所述的...
【专利技术属性】
技术研发人员:叶孙龙,
申请(专利权)人:句容市百诚活性炭有限公司,
类型:发明
国别省市:江苏,32
还没有人留言评论。发表了对其他浏览者有用的留言会获得科技券。