The invention discloses a fur degreasing process, which comprises the following steps: the first step is to soak in water, prepare warm water, add 0.1 \u2011 0.2% Stahl leather probiotic biochemical material, stir evenly, soak the skin in water for 3 \u2011 5h, control the temperature at 34 \u2011 38 \u2103, and control the pH value at 7 \u2011 7.3; the second step is to wash the skin with water, and then wash the skin with water; the third step is to remove the meat, and remove the meat with steel wire roller Remove the meat by machine; step 4: degrease, soak the skin in 35 \u2011 38 \u2103 water, add 0.2 \u2011 0.4% Stahl leather probiotics by mass, for 3 \u2011 4 hours, degrease. The process is environmentally friendly and has good degreasing effect.
【技术实现步骤摘要】
一种毛皮脱脂工艺
:本专利技术涉及皮草制作领域,具体讲是一种毛皮脱脂工艺。
技术介绍
:现有技术中,毛皮脱脂,通常是把皮泡入36-38℃的水中,加盐、杀菌剂、脱脂剂、渗透剂、油脂分散剂等进行脱脂处理,其中杀菌剂普遍采用甲醛,这种脱脂方法为达到较好的脱脂效果,各种助剂和盐的使用量都很大,造成脱脂水中含盐量高,污水处理难度大,COD、BOD指标高,且通常含有APEO和NPEO,对环境影响大,而且现有技术的脱脂方法对柔软度和稳定性上较难进行质量把控。
技术实现思路
:本专利技术所要解决的技术问题是提供一种环保的毛皮脱脂工艺。本专利技术的技术解决方案是,提供一种毛皮脱脂工艺,它包括以下步骤:第一步,浸水、准备常温水,加入0.1-0.2%的的STAHL皮革益生菌生物化料,并搅拌均匀,把皮泡入水中3-5h,温度控制在34-38℃,pH值控制在7-7.3;第二步,水洗,出皮后水洗干净;第三步,去肉,用钢丝辊去肉机去肉;第四步,脱脂,把皮泡入35-38℃的水中,加入质量百分比为0.2-0.4%的STAHL皮革益生菌生物化料,时间为3-4小时,进行脱脂。作为优选,第一步中的STAHL皮革益生菌生物化料为Prosoak皮革益生菌生物化料。作为优选,第四步中的STAHL皮革益生菌生物化料为Prodegreaze皮革益生菌生物脱脂助剂。与现有技术相比,本专利技术具有以下技术效果,由于STAHL皮革益生菌生物化料不含APEO和NPEO,不含酶,分子微小 ...
【技术保护点】
1.一种毛皮脱脂工艺,其特征在于:它包括以下步骤:/n第一步,浸水、准备常温水,加入0.1-0.2%的的STAHL皮革益生菌生物化料,并搅拌均匀,把皮泡入水中3-5h,温度控制在34-38℃,pH值控制在7-7.3;/n第二步,水洗,出皮后水洗干净;/n第三步,去肉,用钢丝辊去肉机去肉;/n第四步,脱脂,把皮泡入35-38℃的水中,加入质量百分比为0.2-0.4%的STAHL皮革益生菌生物化料,时间为3-4小时,进行脱脂。/n
【技术特征摘要】
1.一种毛皮脱脂工艺,其特征在于:它包括以下步骤:
第一步,浸水、准备常温水,加入0.1-0.2%的的STAHL皮革益生菌生物化料,并搅拌均匀,把皮泡入水中3-5h,温度控制在34-38℃,pH值控制在7-7.3;
第二步,水洗,出皮后水洗干净;
第三步,去肉,用钢丝辊去肉机去肉;
第四步,脱脂,把皮泡入35-38℃的水中,加入质量百分比为0.2-...
【专利技术属性】
技术研发人员:沈国清,陆健,董荣华,吕垠,姜苏杰,
申请(专利权)人:桐乡市鑫诺皮草有限公司,嘉兴市皮毛和制鞋工业研究所,
类型:发明
国别省市:浙江;33