Sulfur removal and denitrification aid, including the following mass ratio of raw materials: carbonyl two amine: 5, 8 copies, 5 potassium hypochlorite, 8 parts, titanium dioxide: 2 4 copies, 1 calcium 3, 0.5 calcium oxide, 1, manganese dioxide: 1 2, fatty alcohol polyoxyethylene ether sulfate : 0.5, 2 copies, clay: 1, 3 copies. The invention can reduce the ignition point of coal by adding a small amount of liquid coal combustion agent in the combustion coal, which can reduce the activation energy of the carbon oxidation reaction through the action of permeation, catalysis, oxidation and exchange of metal ions. The invention selects sulfur fixing technology to compounded calcium series, sodium series and ammonia series inorganic materials, and the selected materials have many functions, such as sulfur removal, nitrate removal and carbon sequestration.
【技术实现步骤摘要】
除硫脱硝助燃剂
本专利技术属于助燃剂领域,特别是涉及一种除硫脱硝助燃剂。
技术介绍
建国以来,煤炭在我国一次能源消费构成中占75%左右,预计到2050年这一比例仍将高达50%以上。在一个较长的时期内,煤炭仍将在我国能源利用领域处于主导地位。因此合理利用煤炭资源,提高煤炭的燃烧效率,不仅具有较高的经济效益,同时也具有重大的社会意义。而目前使用燃煤助燃剂是提高煤炭燃烧效率的主要途径。
技术实现思路
本专利技术的目的在于提供一种催化助燃效率高、安全环保的燃煤助燃剂。本专利技术的目的及解决其技术问题是采用以下技术方案来实现。依据本专利技术提出的除硫脱硝助燃剂,包括以下质量份比的原料:碳酰二胺:5-8份,次氯酸钾:5-8份,二氧化钛:2-4份,铁粉:1-3份,氧化钙:0.5-1份,二氧化锰:1-2份,脂肪醇聚氧乙烯醚硫酸钠:0.5-1.5份,高锰酸钾:0.1-0.5份,氧化铁:0.5-2份,粘土:1-3份。较佳的,所述的除硫脱硝助燃剂包括以下质量份比的原料:碳酰二胺:6份,次氯酸钾:6份,二氧化钛:3份,铁粉:2份,氧化钙:1份,二氧化锰:1份,脂肪醇聚氧乙烯醚硫酸钠:1份,高 ...
【技术保护点】
除硫脱硝助燃剂,其特征在于包括以下质量份比的原料:碳酰二胺:5‑8份,次氯酸钾:5‑8份,二氧化钛:2‑4份,铁粉:1‑3份,氧化钙:0.5‑1份,二氧化锰:1‑2份,脂肪醇聚氧乙烯醚硫酸钠:0.5‑1.5份,高锰酸钾:0.1‑0.5份,氧化铁:0.5‑2份,粘土:1‑3份。
【技术特征摘要】
1.除硫脱硝助燃剂,其特征在于包括以下质量份比的原料:碳酰二胺:5-8份,次氯酸钾:5-8份,二氧化钛:2-4份,铁粉:1-3份,氧化钙:0.5-1份,二氧化锰:1-2份,脂肪醇聚氧乙烯醚硫酸钠:0.5-1.5份,高锰酸钾:0.1-0.5份,氧化铁:0.5-2份...
【专利技术属性】
技术研发人员:裴晓辉,周军州,袁波,
申请(专利权)人:洛阳名力科技开发有限公司,
类型:发明
国别省市:河南,41