The invention relates to the technical field of wool socks, in particular to a wool material and a preparation method thereof. The woolen material of the present invention is made of the following raw material of weight percentage: 30 wool 60%, 30 acrylic fiber 60% and 10 polyamide 20%, the wool is a shrink proof and mercerized wool. The woolen material and the preparation method of the present invention are made in a reasonable proportion combination, at the same time, the wool is shrink proof and mercerized, so that it can ensure the natural, soft, warm, moisture absorption and the proper wool feeling of the wool products, and ensure the fastness of the socks, avoid the prickling feeling in the wear, and continue to expand the wool socks. Wear the season.
【技术实现步骤摘要】
一种羊毛料及其制备方法
本专利技术涉及羊毛袜品
,具体涉及一种羊毛料及其制备方法。
技术介绍
中国作为袜子生产大国,正在寻求向“袜子强国”过渡,高质量的袜子产品显然是实现这一过渡的最有效途径。现有袜子产品大都由棉质材料制成,保暖和高档感仍然欠缺。羊毛料具有天然、柔暖、吸湿和高档感,其主要应用于冬季保暖服饰产品,随着人们生活水平的提高,像羊毛料这样天然且高档的服饰料越来越受到市场的欢迎。如果将羊毛料引入袜子产品,羊毛料天然的优势性能显然能提高袜子产品的质量,但又会引入刺痛感强的问题,具体来讲,羊毛料本身具有牢度大的特点,不同于其他服饰并不直接接触人体皮肤,比如羊毛外套,羊毛外套穿着时,人身与羊毛外套之间还隔有内衣或其他衣服,袜子产品是贴身的,牢度大的羊毛料会直接刺痛脚和腿的皮肤。因此,如何制得兼具高档感和舒适感的袜子产品并非易事。
技术实现思路
本专利技术的目的在于针对现有技术中的不足,而提供一种羊毛料及其制备方法,采用该羊毛料和该制备方法制得的羊毛袜兼具高档感和舒适感。为实现上述目的,本专利技术采取的技术方案为:一种羊毛料,所述羊毛料由以下重量百分比的原料制成: ...
【技术保护点】
一种羊毛料,其特征在于,所述羊毛料由以下重量百分比的原料制成:羊毛30‑60%、腈纶30‑60%和锦纶10‑20%,所述羊毛为经过防缩和丝光处理过的羊毛。
【技术特征摘要】
1.一种羊毛料,其特征在于,所述羊毛料由以下重量百分比的原料制成:羊毛30-60%、腈纶30-60%和锦纶10-20%,所述羊毛为经过防缩和丝光处理过的羊毛。2.如权利要求1所述羊毛料,其特征在于,所述羊毛料由以下重量百分比的原料制成:羊毛30%、腈纶60%和锦纶10-20%。3.如权利要求1所述羊毛料,其特征在于,所述羊毛料由以下重量百分比的原料制成:羊毛60%、腈纶30%和锦纶10-20%。4.一种羊毛料,其特征在于,所述羊毛料由以下重量百分比的原料制成:羊毛10%、棉80%和锦纶10-20%,所述羊毛为经过防缩和丝光处理过的羊毛。5.一种如权利要求1-4任一项所述羊毛料的制...
【专利技术属性】
技术研发人员:孙毅仁,张爱萍,杨皓,
申请(专利权)人:上海艾谷针纺织品有限公司,
类型:发明
国别省市:上海,31
还没有人留言评论。发表了对其他浏览者有用的留言会获得科技券。