The invention relates to a preparation method, a special CNC machine tool lubricants are as follows: (1) preparation of base oil, mixed poly olefin a PAO base oil and oil base oil; (2) preparation of lubricating oil additives, (3) preparation of lubricating oil, the base oil 95 75 lubricating oil additives, 30 40 copies were mixed, mixing time is 2 3H, mixed after obtaining products; more copies are quality copies. The multi step mixing method is adopted to prepare the lubricant. The lubricating oil additive with special composition is added to make the lubricating oil have strong self lubrication performance, and it can reduce the friction and guarantee the lubrication effect very well. The invention has simple preparation process and strong operability.
【技术实现步骤摘要】
一种数控机床专用润滑油的制备方法
本专利技术特别涉及一种数控机床专用润滑油的制备方法。
技术介绍
摩擦磨损是摩擦过程中普遍存在的现象,据统计,世界三分之一以上的一次性能源的损失来自摩擦,因此,减小摩擦与磨损造成的经济损失具有重大的意义。而润滑是降低摩擦、减小或避免磨损的有效技术。
技术实现思路
本专利技术针对上述问题提出了一种数控机床专用润滑油的制备方法。具体的技术方案如下:一种数控机床专用润滑油的制备方法,其特征在于,步骤如下:(1)制备基础油,将聚a烯烃PAO基础油与石油基础油的进行混合,混合质量比例为聚a烯烃PAO基础油:石油基础油=5:1,混合时间为2-3H,混合完成得基础油;(2)制备润滑油添加剂,将β-(3,5-二叔丁基-4-羟基苯基)丙酸正十八碳醇酯10-40份,烷基二苯胺20-30份,β-(3,5-二叔丁基-4-羟基苯基)丙酸异辛酯10-20份进行混合,混合时间1-2h,混合结束后加入亚甲基-双-烷基二硫代氨基甲酸酯10-30份、二(2-乙基己基)二硫代磷酸钼10-15份,磷酸三苯酯3-5份继续混合,混合时间为1.5—3H,混合完成后得到润滑油添加剂, ...
【技术保护点】
一种数控机床专用润滑油的制备方法,其特征在于,步骤如下:(1)制备基础油,将聚a烯烃PAO基础油与石油基础油的进行混合,混合质量比例为聚a烯烃PAO基础油:石油基础油=5:1,混合时间为2‑3H,混合完成得基础油;(2)制备润滑油添加剂,将β‑(3,5‑二叔丁基‑4‑羟基苯基)丙酸正十八碳醇酯10‑40份, 烷基二苯胺20‑30份,β‑(3,5‑二叔丁基‑4‑羟基苯基)丙酸异辛酯 10‑20份进行混合,混合时间1‑2h,混合结束后加入亚甲基‑双‑烷基二硫代氨基甲酸酯10‑30份、二(2‑乙基己基)二硫代磷酸钼10‑15份,磷酸三苯酯3‑5份继续混合,混合时间为1.5—3H, ...
【技术特征摘要】
1.一种数控机床专用润滑油的制备方法,其特征在于,步骤如下:(1)制备基础油,将聚a烯烃PAO基础油与石油基础油的进行混合,混合质量比例为聚a烯烃PAO基础油:石油基础油=5:1,混合时间为2-3H,混合完成得基础油;(2)制备润滑油添加剂,将β-(3,5-二叔丁基-4-羟基苯基)丙酸正十八碳醇酯10-40份,烷基二苯胺20-30份,β-(3,5-二叔丁基-4-羟基苯基)丙酸异辛酯10-20份进行混合,混合时间1-2h,混合结束后加入亚甲基-双-烷...