The utility model discloses a strengthening device of copper slag slow cooling process, has for the package and positioning slag ladle slag bag positioning area slag loading the copper slag, which comprises a bracket, electric hoist and slag insulation cover, wherein the electric hoist is arranged on the bracket, the slag ladle insulation cover a link, the electric hoist and the link point connection. The utility model has the beneficial effect of strengthening the heat preservation effect of the copper slag bag, and effectively promoting the crystallization and growth of copper slag, especially in the open area of slag bag. The device can improve the recovery rate of copper slag from 2 to 5%, and it has simple transformation. It does not need to replace the existing slag package, and does not affect the cooling rate of the copper slag during the water cooling period.
【技术实现步骤摘要】
一种铜渣缓冷过程的强化装置
本技术涉及尾渣资源回收领域,特别涉及一种铜渣浮选回收工艺中含铜相长大强化控制的装置。
技术介绍
铜是国家战略资源,我国是第一大铜消费国,但我国铜资源禀赋差,我国铜原料对外依存度达73%,2015年铜精矿进口量达1329万吨。目前,我国年产铜渣2000余万吨,渣中含有铜、金、银等有价金属近百亿元,提高铜渣资源利用率成为重要的研究方向。铜渣中铜的回收方法主要有选矿(浮选)法、火法贫化法和湿法冶金法。其中,浮选法是目前从铜渣中回收铜金属最有效的方法,具有能耗低、回收率高的特点。影响铜渣浮选的主要因素有以下三个方面,包括冶炼方式、冷却方式、浮选工艺。其中,铜渣冷却方式对炉渣浮选回收的相关指标有重要的影响,铜渣冷却速度的快慢决定了铜矿物的结晶粒度大小。铜颗粒的大小与其嵌布特性是影响铜渣可选性能的关键。因此,采取缓冷措施使铜渣聚集长大形成相对集中的独立相,有利于有价金属的回收。目前,铜渣缓冷工艺在铜冶炼企业广泛使用,一般将高温熔融态铜渣倒入铜渣包后运输至渣缓冷场空冷5~30h,随后进行水冷。由于铜渣中的含铜相结晶温度大致在1050~1280℃之间。 ...
【技术保护点】
一种铜渣缓冷过程的强化装置,具有用于装载所述铜渣的渣包以及定位渣包的渣包定位区,其特征在于,包括支架、电葫芦与渣包保温盖,所述电葫芦设置于所述支架上,所述渣包保温盖设有链接点,所述电葫芦与所述链接点连接。
【技术特征摘要】
1.一种铜渣缓冷过程的强化装置,具有用于装载所述铜渣的渣包以及定位渣包的渣包定位区,其特征在于,包括支架、电葫芦与渣包保温盖,所述电葫芦设置于所述支架上,所述渣包保温盖设有链接点,所述电葫芦与所述链接点连接。2.根据权利要求1所述的铜渣缓冷过程的强化装置,其特征在于,所述渣包保温盖由外层与内层构成,所述外层为铸铁层,所述内...
【专利技术属性】
技术研发人员:陈杭,王俊娥,吴健辉,衷水平,张焕然,林泓富,李思勇,刘春,廖元杭,周勇华,许培燕,熊家春,
申请(专利权)人:紫金铜业有限公司,
类型:新型
国别省市:福建,35
还没有人留言评论。发表了对其他浏览者有用的留言会获得科技券。