The invention discloses a method for producing refined crude selenium selenium, selenium oxide and two high purity selenium free rinsing method without water rinse, only need to add one or more than two kinds of alkali in crude selenium in acid neutralization; it includes two steps: (1) analysis of acid content assay of crude selenium, determination of crude selenium added alkali; (2) the crude selenium and required adding alkali into the material mixer, after mixing, discharging standby. The process of the invention is very simple, according to the amount of added mixing alkali and crude selenium, do not need to use a lot of water to rinse, not only simplifies the process and shorten the production cycle, it is more important to avoid a lot of waste water, obviously reduces the production cost, the more important is that acid treatment effect of selenium is very crude well, compared with the method of water rinse, while significantly reducing the cost and significantly enhance the effect.
【技术实现步骤摘要】
一种利用粗硒生产精硒、二氧化硒和高纯硒的免漂洗前处理方法
本专利技术涉及一种利用粗硒生产精硒、二氧化硒和高纯硒的免漂洗前处理方法,属于节能减排和环境保护领域。
技术介绍
我国是硒的生产量和用量最大的国家,硒属于稀有贵金属,伴生于铜、铅等矿床中。粗硒一般来源于电解铜阳极泥的加工处理,由于其生产工艺的原因,粗硒产品一般都含有一定量的硫酸;而在精硒、二氧化硒和高纯硒的生产过程中,需要加温升华或氧化,使单质硒升华提纯或氧化为二氧化硒;如果粗硒中含有硫酸,在加热过程中,一是会对设备产生严重的腐蚀,二是硫酸雾会严重污染环境,三是对产品质量造成很大影响;因此,现有工艺在用粗硒生产精硒、二氧化硒和高纯硒前,一般要对粗硒进行漂洗,以洗掉其酸含量,但要漂洗到中性是十分困难的,在这个过程中,漂洗一吨粗硒需要消耗5-10吨清水,漂洗水不仅含有酸(一般pH为3左右),还含有大量的其他污染物和贵金属,如砷、硒、镉、锑、铜、锌、镍、铅等重金属污染物,以及硒、银等贵金属;特别是砷和硒的浓度可达几十到上百毫克/升;这种多种重金属的复合污染,不仅治理难度大,而且治理成本很高,由于工艺复杂,很难做到稳 ...
【技术保护点】
一种利用粗硒生产精硒、二氧化硒和高纯硒的免漂洗前处理方法,其特征在于,无需用水漂洗,只需在粗硒中加入一种或两种以上的碱性化合物即碱进行酸中和即可;其处理工艺包括两个步骤:(1)分析化验粗硒的酸含量,确定粗硒需加入的碱量即碱性化合物的量;(2)将粗硒与所需加入的碱放入物料混合器中,充分混合后,出料备用。
【技术特征摘要】
1.一种利用粗硒生产精硒、二氧化硒和高纯硒的免漂洗前处理方法,其特征在于,无需用水漂洗,只需在粗硒中加入一种或两种以上的碱性化合物即碱进行酸中和即可;其处理工艺包括两个步骤:(1)分析化验粗硒的酸含量,确定粗硒需加入的碱量即碱性化合物的量;(2)将粗硒与所需加入的碱放入物料混合器中,充分混合后,出料备用。2.根据权利要求1所述的利用粗硒生产精硒、二氧化硒和高纯硒的免漂洗前处理方法,其特征在于,所述的碱为碳酸钠、氢氧化钠、氧化钙、氢氧化钙...