The invention discloses a method for P204 extraction of nickel loaded organic removal of ammonia, which comprises the following steps: A, preparing nickel salt solution containing nickel ion 30g/L 50g/L; B, P204 extract nickel supported nickel salt solution mixed organic and step A, the P204 extraction nickel loaded with machine after washing phase the use of nickel salt solution obtained after washing ammonia P204 extraction of nickel loaded organic; C, acid stripping ammonia washing after P204 extraction of nickel loaded organic, nickel stripping solution. The invention is organic to wash P204 extraction by nickel supported nickel salt solution containing nickel ion 30g/L 50g/L, Ni nickel salt solution in the washing process
【技术实现步骤摘要】
一种P204萃镍负载有机脱除氨的方法
本专利技术属于湿法冶金
,具体涉及一种P204萃镍负载有机脱除氨的方法。
技术介绍
由于氨水具有挥发性,便于后续回收利用,因此,在萃取镍时采用氨皂代替钠皂逐步得到应用。特别是在P204萃取镍时,采用氨水皂化有机,萃取结束后会有一部分氨残留在负载有机上,反萃时进入反萃液,进而影响产品质量。采用传统的降低皂化率和酸洗等方法,反萃液中氨含量均在8g/L左右,达不到降低反萃液中氨含量的目的。
技术实现思路
本专利技术的目的是为了解决现有技术中存在的技术问题,提供一种简单有效、流程短且能保证得到纯净反萃液的P204萃镍负载有机脱除氨的方法。为了达到上述目的,本专利技术采用以下技术方案:一种P204萃镍负载有机脱除氨的方法,该方法包括以下步骤:A、配制含镍离子30g/L-50g/L的镍盐溶液;B、将P204萃镍负载有机与步骤A中配制的镍盐溶液混合,利用镍盐溶液对P204萃镍负载有机进行洗涤后分相,得到洗氨后P204萃镍负载有机;C、用酸反萃洗氨后P204萃镍负载有机,得到镍反萃液。进一步地,所述步骤B中洗涤时洗涤相比O/A为5-12:1、级数为2-10级逆流、洗涤时间为2-10min、洗涤温度为20℃-40℃。进一步地,所述步骤A中镍盐溶液为硫酸镍、氯化镍、硝酸镍溶液中的一种。进一步地,所述步骤C中酸为盐酸或硫酸。进一步地,所述步骤C中反萃时采用四级逆流反萃。本专利技术相对现有技术具有以下有益效果:本专利技术通过含镍离子30g/L-50g/L的镍盐溶液对P204萃镍负载有机进行洗涤,洗涤过程中镍盐溶液中的Ni2+将P204萃镍负 ...
【技术保护点】
一种P204萃镍负载有机脱除氨的方法,其特征在于该方法包括以下步骤:A、配制含镍离子30g/L‑50g/L的镍盐溶液;B、将P204萃镍负载有机与步骤A中配制的镍盐溶液混合,利用镍盐溶液对P204萃镍负载有机进行洗涤后分相,得到洗氨后P204萃镍负载有机;C、用酸反萃洗氨后P204萃镍负载有机,得到镍反萃液。
【技术特征摘要】
1.一种P204萃镍负载有机脱除氨的方法,其特征在于该方法包括以下步骤:A、配制含镍离子30g/L-50g/L的镍盐溶液;B、将P204萃镍负载有机与步骤A中配制的镍盐溶液混合,利用镍盐溶液对P204萃镍负载有机进行洗涤后分相,得到洗氨后P204萃镍负载有机;C、用酸反萃洗氨后P204萃镍负载有机,得到镍反萃液。2.根据权利要求1所述的一种P204萃镍负载有机脱除氨的方法,其特征在于:所述步骤B中洗涤时洗涤相比O/A为5-...
【专利技术属性】
技术研发人员:刘玉强,李尚勇,张晗,陈彩霞,李全,张树峰,李娟,李维舟,田忠元,欧晓健,朱锐伦,席海龙,高晓婷,王书友,张娟,郁洪波,孔令军,马天飞,
申请(专利权)人:金川集团股份有限公司,
类型:发明
国别省市:甘肃,62