The present invention discloses a novel nano rubber glue, according to the weight consists of the following components: nano titanium dioxide 6 12 copies, 30 copies of the 20 silicone rubber, nano titanium dioxide 5 10 copies, 15 copies of urea formaldehyde resin 8, benzene two amine 1 5 mineral oil, 2 6, 8, 4 propylene glycol formaldehyde 2 6 copies, 3 copies, 1 sodium hydroxide oxidation water 50 30. Compared with the prior art, the special nano materials added in the formulation process, the bonding performance of rubber glue has improved dramatically, nano TiO2, thereby reducing agglomeration reaction, make rubber glue with high performance durable, not only improve the use effect, but also effectively reduces the glue the dosage, reduce the use of cost.
【技术实现步骤摘要】
一种新型纳米橡胶胶水
本专利技术具体涉及一种新型纳米橡胶胶水。
技术介绍
现有的橡胶胶水的粘结性能以及粘结效果的持久性不是很突出,因此无法适用于一些对于粘结性以及粘结持久性要求比较高的行业领域进行使用。
技术实现思路
专利技术目的:为了克服现有技术中存在的不足,提供一种粘结性能好且粘结效果持续时间非常长的新型纳米橡胶胶水。技术方案:为实现上述目的,本专利技术提供一种新型纳米橡胶胶水,按重量份数由以下组份组成:纳米钛白粉6-12份、有机硅橡胶20-30份、纳米二氧化钛5-10份、脲醛树脂8-15份、间苯二胺1-5份、矿物油2-6份、丙二醇4-8份、甲醛2-6份、氢氧化钠1-3份、氧化水30-50份。进一步地,按重量份数由以下组份组成:纳米钛白粉6-7份、有机硅橡胶20-22份、纳米二氧化钛5-6份、脲醛树脂8-9份、间苯二胺1-2份、矿物油2-3份、丙二醇4-5份、甲醛2-3份、氢氧化钠1-2份、氧化水30-35份。进一步地,按重量份数由以下组份组成:纳米钛白粉10-12份、有机硅橡胶28-30份、纳米二氧化钛9-10份、脲醛树脂14-15份、间苯二胺4-5份、矿物油5 ...
【技术保护点】
一种新型纳米橡胶胶水,其特征在于:按重量份数由以下组份组成:纳米钛白粉6‑12份、有机硅橡胶20‑30份、纳米二氧化钛5‑10份、脲醛树脂8‑15份、间苯二胺1‑5份、矿物油2‑6份、丙二醇4‑8份、甲醛2‑6份、氢氧化钠1‑3份、氧化水30‑50份。
【技术特征摘要】
1.一种新型纳米橡胶胶水,其特征在于:按重量份数由以下组份组成:纳米钛白粉6-12份、有机硅橡胶20-30份、纳米二氧化钛5-10份、脲醛树脂8-15份、间苯二胺1-5份、矿物油2-6份、丙二醇4-8份、甲醛2-6份、氢氧化钠1-3份、氧化水30-50份。2.根据权利要求1所述的一种新型纳米橡胶胶水,其特征在于:按重量份数由以下组份组成:纳米钛白粉6-7份、有机硅橡胶20-22份、纳米二氧化钛5-6份、脲醛树脂8-9份、间苯二胺1-2份、矿物油2-3份、丙二醇4-5份、甲醛2-3份、氢氧化钠1-2份、氧化水30-35份。3.根据权利要求1所述的一种新型纳米橡胶胶水,其特征在于:按重量份数由以下组份组成:纳米钛白粉10-12份、有机硅橡胶28-30份、...