The utility model discloses a brick compressive clamp, involving compressive strength testing tools, including the compression plate top pressure device, a clamping arm, a connecting plate and placed in the pressure testing machine, the jacking device comprises a bearing plate, pressure plate and dowel bar, the connecting in the center position is arranged for receiving the dowel hole, both ends of the connecting plate through a hinge with prestressed symmetrical connecting the clamp arm, the clamp arm is provided with an upper rocker and the bottom in width between the plate and the two pinch phase adaptation. Not pressed, the clamping arm, the compression arm open, pressure by the top pressure is transferred to the sample, which can be clamped, and does not affect the test data, and improves the test efficiency, solve the existing technology in sintering brick non specimen molding sample preparation are prone to confusion, effect of test group sample separation, the problem of efficiency.
【技术实现步骤摘要】
一种烧结普通砖抗压夹具
本技术涉及烧结普通砖抗压强度检测辅助工具领域,尤其涉及烧结普通砖抗压强度检测试样夹持工具领域,具体的说,是一种烧结普通砖抗压夹具。
技术介绍
烧结普通砖的抗压强度试验中,试样的制备方式有一次成型制样、二次成型制样、非成型制样这三种。一次成型制样是指,将烧结普通砖样品从中间锯成两个半截砖,将已切开的两个半截砖放入室温的净水中浸20min~30min后取出,在铁丝网架上滴水20min~30min,以断口相反方向装入制样模具中,用插板控制两个半砖间距不应大于5mm,砖大面与模具间距不应大于3mm,砖断面、顶面与模具间垫以橡胶垫或其他密封材料,再将装好试样的模具置于振动台上,加入适量搅拌均匀的净浆,振动0.5min~1min后静置,达到初凝后拆模;二次成型制样是指,将整块烧结普通砖样品放入室温的净水中浸20min~30min后取出,在铁丝网架上滴水20min~30min,向模具内加入适量搅拌均匀的净浆,将整块试样一个承压面与净浆接触、装入制样模具中,再将模具置于振动台上,振动0.5min~1min后静置,达到初凝后拆模,得到一个承压面的找平层,再按 ...
【技术保护点】
一种烧结普通砖抗压夹具,其特征在于,包括顶压器(1)、夹臂(2)、连接板(3)和安置在压力试验机上的受压板(4),所述顶压器(1)包括承压板(11)、压力板(13),以及固定连接或一体成型在所述承压板(11)与所述压力板(13)之间的传力杆(12),所述连接板(3)中心位置开设有用于容纳所述传力杆(12)的洞口,所述连接板(3)两端通过带预应力的铰接件(22)对称连接有两个所述夹臂(2),所述夹臂(2)中部形成用于夹持试样的空腔,所述夹臂(2)的上部和下部分别设置有一体成型的翘板(21)和夹脚(23),所述翘板(21)位于所述铰接件(22)上部、所述承压板(11)和压力板( ...
【技术特征摘要】
1.一种烧结普通砖抗压夹具,其特征在于,包括顶压器(1)、夹臂(2)、连接板(3)和安置在压力试验机上的受压板(4),所述顶压器(1)包括承压板(11)、压力板(13),以及固定连接或一体成型在所述承压板(11)与所述压力板(13)之间的传力杆(12),所述连接板(3)中心位置开设有用于容纳所述传力杆(12)的洞口,所述连接板(3)两端通过带预应力的铰接件(22)对称连接有两个所述夹臂(2),所述夹臂(2)中部形成用于夹持试样的空腔,所述夹臂(2)的上部和下部分别设置有一体成型的翘板(21)和夹脚(23),所述翘板(21)位于所述铰接件(22)上部、所述承压板(11)和压力板(13)之间,所述夹脚(23)位于所述夹臂(2)底部,所述受压板(4)与两个所述夹脚(23)中间的宽度相适应。2.根据权利要求1所述的一种烧结普通砖抗压夹具,其特征在于,所述夹脚(23)宽度为5mm,所述受压板(4)的长度...