The invention discloses a three methyl silicon alkoxide preparation method and application of preparation steps for six methyl siloxane and two potassium hydroxide as 10L three alcohol preparation bottle, add 10ml, heated to reflux for 48 hours by a water separator, and water, cooling, filtering, drying, obtained white solid three methyl silicon potassium alkoxide. The present invention uses a cheap raw material for industrial production, six methyl two siloxane (MM) as raw material, and a high content of three methyl silicon potassium by heating and refluxing reaction under various catalysts of potassium hydroxide. These catalysts are favorable for the dissolution of potassium hydroxide and are favorable for the reaction.
【技术实现步骤摘要】
一种三甲基硅醇盐的制备方法及应用
本专利技术涉及
,具体为一种三甲基硅醇盐的制备方法及应用。
技术介绍
有机硅醇和有机硅醇盐在合成硅油、树脂和硅橡胶领域有着非常广泛和重要的意义,尤其在新产品改性方面,近年来的研究有了比较大的突破。因此,对有机硅醇和硅醇盐的合成研究有着非常重要的意义。三甲基硅醇钾是其中最重要的一种。在现有技术中,这类三甲基硅醇钾的做法主要有:1)以工业基础原料三甲基氯硅烷为原料,制备三甲基硅醇,再跟金属钾反应得到三甲基硅醇钾,这种方法这种方法再制备三甲基硅醇时非常不容易控制,三甲基硅醇非常不稳定,控制不好全部生产六甲基二硅氧烷,第二步用到金属钾,非常危险,不利于工业化,而且再第二步反应中控制不好业很容易得到六甲基二硅氧烷。2)以六甲基二硅氧烷和氨基钠做原料,直接反应得到产品,这个方法虽然简单,但是氨基钠非常危险,而且比较昂贵,不适合工业化生产。3)以六甲基二硅氧烷和甲基理做原料,直接反应得到产品,这个方法虽然简单,但是甲基理非常危险,而且比较昂贵,反应需要低温无水无氧,条件比较苛刻,不适合工业化生产。
技术实现思路
本专利技术的目的在于提供一种简 ...
【技术保护点】
一种三甲基硅醇盐的制备方法,其特征在于:制备步骤为将六甲基二硅氧烷和氢氧化钾至于10L的三口瓶中,加入10ml的醇类制剂,加热回流48小时,同时用分水器分水,冷却,过滤,干燥,得到白色固体三甲基硅醇钾。
【技术特征摘要】
1.一种三甲基硅醇盐的制备方法,其特征在于:制备步骤为将六甲基二硅氧烷和氢氧化钾至于10L的三口瓶中,加入10ml的醇类制剂,加热回流48小时,同时用分水器分水,冷却,过滤,干燥,得到白色固体三甲基硅醇钾。2.根据权利要求1所述的一种三甲基硅醇盐的制备方法,其特征在于:所述醇类制剂为甲醇、乙醇、异丙醇或乙二醇。3.一种权利要求1所述的三甲基硅醇盐的应用,其特征在于:所述三甲基硅醇钾置于2L无水四氢呋喃中,搅拌下滴加二甲基氯硅烷,滴完,室温下反应1h,过滤,浓缩,乙醚萃取,干燥,浓缩,得到纯度大于98%的五甲基二硅氧烷。4.一种权利要求1所述的三甲基硅醇盐的应用,其特征在于:所述三甲基硅醇...
【专利技术属性】
技术研发人员:杨绍祖,韦举志,王欢,李长斌,
申请(专利权)人:壮铭新材料科技江苏有限公司,
类型:发明
国别省市:江苏,32
还没有人留言评论。发表了对其他浏览者有用的留言会获得科技券。