The name of the invention is light and the air bubble chloride drum production of modified chlorinated paraffin 70 method, which belongs to the technical field of chlorinated paraffin, chlorinated paraffin 70 in order to improve the production rate of the original 87106851.6 patent technology improved the solution is still adding source based on the 87106851.6 device is added on the other vessel bubbler chlorine gas directly into the bubble, between the part and the agitation for series cycle heat exchanger, the raw material of paraffin wax is heated to a certain temperature (110 degrees Celsius), and then according to a certain proportion (about 5%) adding polyethylene is melted by heating, and then put the kettle to heat and chloride, ensure the molten polyethylene, production method faster.
【技术实现步骤摘要】
光氯化鼓泡鼓动气冷热法生产改性氯化石蜡-70方法(一)
:本专利技术涉及一种生产改性氯化石蜡-70的方法。(二)
技术介绍
:“强制循环鼓动法生产氯化石蜡装置”(原专利号:87106851.6)其技术方案是:将氯气送入反应釜空间,氯气和反应生成的氯化氢气体抽出,经喷射泵和贮液槽,被水吸收,余下氯气鼓压进鼓动器,如此连续快速反应。但用于生产氯化石蜡速度还不够理想,尤其是生产高氯化石蜡产品,到反应后期,速度趋缓。(三)
技术实现思路
:本专利技术的任务是基于对原87106851.6专利技术专利的一种改进,提供一种更快的生产改性氯化石蜡-70的方法,采取的技术方案是釜内加装上光源,在其反应釜内另加装上鼓泡器,由氯源供应的氯气直接通入鼓泡器,对反应釜物料进行鼓泡。这样在强制循环鼓动下再加上鼓泡提高反应速度。在装置鼓动器与循环部分出口之间串联换热器,对进入鼓动器的反应气体先进行加热或者冷却后通入鼓动器,确保最佳反应温度,把原料石蜡加热到一定温度(110℃左右),然后按一定比例(5%左右)加入聚乙烯进行加热熔化,然后投入釜内氯化,并以热确保聚乙烯为熔化状。(四)具体实施方式:一套“强制循环鼓动法生产氯化石蜡装置”,使用500升反应釜,其反应釜内加装1000瓦汞灯,其反应釜内再加装上现有通行的鼓泡器。用换热面2.5米2的换热器串联在鼓动器与循环部分出口之间,把原料石蜡加热到一定温度(110℃左右),然后按一定比例(5%左右)加入聚乙烯进行加热熔化,然后投入釜内氯化,并以热确保聚乙烯为熔化状。本专利技术操作与“强制循环鼓动法生产氯化石蜡装置”同,料温低,换热器加热,反之冷却。
【技术保护点】
一种光氯化鼓泡鼓动气冷热法生产改性氯化石蜡‑70方法,包括把氯气和氯化氢气体抽出,氯化氢气体在喷射泵和贮液槽被水吸收,余下氯气鼓压进鼓动器,如此连续,其特征是:釜内装有光源氯化氯气直接放入釜内鼓泡器,鼓动器与循环部分出口之间串联换热器,对反应气体加热或冷却,把原料石蜡加热到一定温度(110℃左右),然后按一定比例(5%左右)加入聚乙烯进行加热熔化,然后投入釜内氯化,并以热确保聚乙烯为熔化状。
【技术特征摘要】
1.一种光氯化鼓泡鼓动气冷热法生产改性氯化石蜡-70方法,包括把氯气和氯化氢气体抽出,氯化氢气体在喷射泵和贮液槽被水吸收,余下氯气鼓压进鼓动器,如此连续,其特征是:釜内装有光源氯化氯气直接放入釜内鼓...