一种基于三维针尖状氮化碳的微量铜离子光电化学检测方法技术

技术编号:22593364 阅读:40 留言:0更新日期:2019-11-20 10:25
本发明专利技术属于环境监测技术领域,提供一种基于三维针尖状氮化碳的微量铜离子光电化学检测方法。通过离子热方法,掺入共融盐对原始氮化碳进行二次热处理,结合冰水淬火措施形成三维分支结构,且分支向外辐射,顶端呈类针尖状。利用电泳沉积法制备3DBC‑C

A photoelectrochemical detection method for trace copper based on three-dimensional needle like carbon nitride

The invention belongs to the technical field of environmental monitoring, and provides a micro copper ion photoelectrochemical detection method based on three-dimensional needle like carbon nitride. In this paper, the original carbon nitride was treated by the method of ion heat treatment and co melting salt. Combined with ice water quenching, the three-dimensional branch structure was formed. The branch radiated outwards and the top of the branch was needle like. Preparation of 3DBC \u2011 C by electrodeposition

【技术实现步骤摘要】
一种基于三维针尖状氮化碳的微量铜离子光电化学检测方法
本专利技术属于环境监测
,涉及一种基于三维针尖状氮化碳的微量铜离子光电化学传感检测方法。
技术介绍
随着我国工业的不断发展,空气、水、土壤均受到了重金属离子污染。重金属污染与其它有机化合物的污染不同,前者具有富集性的特点使其难以在环境中被降解,进入生态系统后就会存留、积累和迁移,从而造成危害。而且,金属的有利或有害不仅取决于金属的种类、理化性质,而且还取决于金属存在的浓度及化学形态,即便有益的金属元素若浓度超过某一标准值也会使动植物中毒,甚至死亡。重金属离子一旦被人体吸收就会与体内的蛋白质及各种酶发生强烈的相互作用,微量的重金属离子不会对人体造成伤害,但如果体内重金属离子浓度过高,会改变酶的立体结构、活性中心的电荷或替换酶中的其它必需金属离子,使酶失活。此外,也可能在人体的某些器官中富集,如果超过人体所能耐受的限度,会对人体产生极大的毒害作用,例如众所周知的“水俣病”就是由食用的鱼中含有氯化甲基汞引起的,“骨痛病”则由镉污染引起。因此,监测有毒金属离子是环境保护和疾病预防、治疗的重要问本文档来自技高网...

【技术保护点】
1.一种基于三维针尖状氮化碳的微量铜离子光电化学检测方法,其特征在于,步骤如下:/n(1)制备三维针尖状氮化碳;/n(2)3DBC-C

【技术特征摘要】
1.一种基于三维针尖状氮化碳的微量铜离子光电化学检测方法,其特征在于,步骤如下:
(1)制备三维针尖状氮化碳;
(2)3DBC-C3N4/FTO光电极的制备:将步骤(1)得到的三维针尖状氮化碳加入到异丙醇中,三维针尖状氮化碳在异丙醇中的浓度为0.15~0.5g/L,同时加入硝酸镁,硝酸镁的终浓度≤10g/L,混合均匀,获得电泳沉积溶液;在两电极电化学体系中,将FTO导电玻璃片作为工作电极,铂丝电极作为对电极浸入上述沉积溶液中,沉积时间为3~5分钟,电压为80~10...