The sandwich compound environment-friendly and energy-saving combustion-supporting agent provides environment-friendly and energy-saving coal combustion-supporting agent. The product is made of eight kinds of chemical raw materials, ferrocene and magnesium powder. The production process of the sandwich compound environment-friendly and energy-saving combustion-supporting agent is as follows: crushing and sieving raw materials, weighing well, mixing evenly in turn, etc. The product has reasonable formula, simple equipment, simple process, low cost and convenient use. It can save fuel, eliminate smoke, dust and desulfurize.
【技术实现步骤摘要】
环保节能助燃剂及其生产工艺
:本专利技术夹心化合物环保节能助嫩剂及其生产工艺属专门用于各类工业锅炉、粉煤炉、窑炉及民用蜂窝煤炉所用煤炭燃料助燃剂及其生产工艺,尤其沙及一种夹心化合物节能助燃剂配方及其生产工艺。
技术介绍
:目前企业生产销售的煤炭助燃剂单一从供氧角度出发,瞬间作用强,但持续性较短,有机化合物含量少,使煤炭中可燃物质得不到充分燃烧,热效率得不到充分利用,烟气中硫化物及有害气体排放量超标。
技术实现思路
:本专利技术夹心化合物环保节能助燃剂不仅生产工艺简便,而且在配方中科学选择原料,定量准确,混合生产程序合理,使各原料均匀混合起来,在煤炭燃烧过程中各种化合物随燃烧温度的升高而逐渐发生作用,气化作用明显,助燃持续时间长,克服了传统煤炭助燃剂瞬间释放氧气这一敞端,并在燃烧中膨化、氧化、气化同步进行,使煤炭中高分子化合物得到充分裂解、燃烧,能量得到充分释放。含夹心化合物升华友盖燃烧面,大大减少烟气中硫含量,降低了林格曼黑度级,有效地节约了煤炭,减少了环境污染。为了实现上述专利技术目的,其夹心化合物环保节能煤炭助燃剂及其生产工艺如下所述:l、夹心化合物环保节能助燃剂主要由二茂铁、镁粉、硝竣钾、硝政铅、有机化合物、氛化钠、活性土和氧化,.J八种类化工原料组成,夹心化合物环保节能助燃剂有效配方量、有效百分比含量如下表所示:2、夹心化合物环保节能助燃剂生产工艺如下:(l)按配方量将原料分别称齐并粉碎,过60目筛备用。(2)将二茂铁和镁粉放入木制容器中用木铣搅拌均匀。(3)将硝酸钾和峭竣铅放入木制搅拌机中挽拌均匀。(4)将搅拌好的(2)加入(3)中搅拌均匀.(5)将 ...
【技术保护点】
1.本专利技术夹心化合物环保节能助燃剂及其生产工艺特征在于夹心化合物环保节能助燃剂由二茂铁、镁粉、硝酸钾、硝酸铅、有机化合物、熟化钠、活性土和氧化剂八种类化工原杆配方组成,生产夹心化合物节能煤炭助燃剂的工艺如下所述:生产前分别将原料粉碎过50目筛后按配方量称齐,先将二茂铁同镁粉、硝酸钾同硝酸铅分别搅拌均匀后再混合挽拌均匀,随后依次将有机化合物、氧化剂活性土、熟化钠和氧化剂分别加入挽拌均匀后成产品。
【技术特征摘要】
1.本发明夹心化合物环保节能助燃剂及其生产工艺特征在于夹心化合物环保节能助燃剂由二茂铁、镁粉、硝酸钾、硝酸铅、有机化合物、熟化钠、活性土和氧化剂八种类化工原杆配方组成,生产夹心化合物节能煤炭助燃剂的工艺如下所述:生产前分别将原料粉碎过50目筛后按配方量称齐,先将二茂铁同镁粉、硝酸钾同硝酸铅分别搅拌均匀后再混合挽拌均...
【专利技术属性】
技术研发人员:丁伟,
申请(专利权)人:绵阳旺通科技有限公司,
类型:发明
国别省市:四川,51