The invention discloses a preparation method of bubble slurry for soil improvement of EPB shield cabin, which comprises the following steps: first, the base slurry is disposed: foaming liquid and slurry are mixed and stirred evenly; then bubble slurry is generated: the base slurry is placed in an airtight or semi-airtight container, and the base slurry is stirred with an agitator to obtain bubble slurry. The bubble slurry prepared by the method provided by the invention has good economy and stability, similar to bentonite slurry, and has the performance of improving fluidity, adjusting strength and reducing permeability coefficient. It is suitable for the improvement of cabin soil of earth pressure shield machine, effectively reducing torque, improving the fluidity and impermeability of cabin soil.
【技术实现步骤摘要】
一种用于土压平衡盾构舱土改良的气泡泥浆制备方法
本专利技术涉及盾构隧道施工
,具体涉及一种用于土压平衡盾构舱土改良的气泡泥浆制备方法。
技术介绍
我国城市轨道交通建设发展迅速,隧道建设工程量日益增加。盾构法隧道施工具有对周边的建筑环境的影响小、施工速度快,施工自动化程度高、安全性好等优点被广泛的采用,尤其是在建筑密集或地层性质特殊的地区。常用的盾构机类型为土压平衡式盾构机(简称土压盾构)和泥水平衡式盾构机(简称泥水盾构)。其中,土压盾构几乎不占用地表面积,施工成本相对较低,广泛应用于城市地铁隧道建设。土压盾构施工中,由于地层的复杂多样,容易发生压力舱闭塞、结饼或排土器排土口喷涌等问题,需要将位于刀盘后方的压力舱内的舱土改良为塑性流动状态,即较高的流动性、较低的渗透性、较好的压缩性,以支护开挖面的土水压力、维持开挖面稳定。目前,国内外常用的舱土改良剂为纯气泡或纯膨润土泥浆。存在的问题是,纯气泡虽然可以较好地改善舱土流动性,但在水压作用下容易从土颗粒孔隙中挤出,对舱土渗透性的改良效果较差;纯膨润土泥浆可以较好地降低舱土渗透性,但是需要大量注入才能达到理想效果,成 ...
【技术保护点】
1.一种用于土压平衡盾构舱土改良的气泡泥浆制备方法,其特征在于:包括以下步骤:(1)配置基浆:将发泡液和泥浆混合搅拌均匀;(2)生成气泡泥浆:将基浆放置在密闭或半密闭容器中,用搅拌器搅拌基浆,得到气泡泥浆。
【技术特征摘要】
1.一种用于土压平衡盾构舱土改良的气泡泥浆制备方法,其特征在于:包括以下步骤:(1)配置基浆:将发泡液和泥浆混合搅拌均匀;(2)生成气泡泥浆:将基浆放置在密闭或半密闭容器中,用搅拌器搅拌基浆,得到气泡泥浆。2.根据权利要求1所述的一种用于土压平衡盾构舱土改良的气泡泥浆制备方法,其特征在于:所述步骤(2)中生成气泡泥浆的具体步骤为:1)将配置好的基浆放置在密闭或半密闭容器中,容器容积至少为基浆体积的30倍;2)用转速2000~5000r/min的搅拌器搅拌基浆,搅拌时间2min,搅拌方式采用框式搅拌机搅拌;3)关闭搅拌机,待容器中的气泡不发生明显的灭泡之后,即制得气泡泥浆。3.根据权利要求1所述的一种用于土压平衡盾构舱土改良的气泡泥浆制备方法,其特征在于:所述步骤(1)配置基浆中,所述发泡液占比0.1...
【专利技术属性】
技术研发人员:朱伟,王璐,钱勇进,王超,徐超,胡涧楠,