The invention provides a foam stamping method with small spacing between two holes, which ensures that the edges of holes with small spacing do not peel off, and ensures the quality of products. There are two groups of uniform foam holes in the thickness direction of foam cotton. They are the first foam hole and the second foam hole. The minimum edge spacing between the first foam hole and the second foam hole is not more than 1 mm. The first foam hole is punched out by the first die, then the first die moves, and the second foam hole is punched out by the second die as a whole, and then the second die moves as a whole.
【技术实现步骤摘要】
一种两孔间距较小的泡棉冲压方法
本专利技术涉及泡棉冲压的
,具体为一种两孔间距较小的泡棉冲压方法。
技术介绍
现有的泡棉冲压时,均采用产品孔一次冲压成型的方法,但是由于有的孔间距较小,此时两种孔同时冲切泡棉会产生形变,进而使得泡棉孔的边缘会和离型膜产生脱壳现象,不能保证产品的品质。
技术实现思路
针对上述问题,本专利技术提供了一种两孔间距较小的泡棉冲压方法,其确保间距较小的孔的边缘不会脱壳,确保产品的品质。一种两孔间距较小的泡棉冲压方法,其特征在于:泡棉的厚度方向设置有两组均布的泡棉孔,分别为第一泡棉孔、第二泡棉孔,所述第一泡棉孔、第二泡棉孔的最小边缘间距不大于1mm,其通过第一刀模整体冲压出第一泡棉孔,之后第一刀模整体上移,通过第二刀模整体冲压出第二泡棉孔,之后第二刀模整体上移。其进一步特征在于:所述泡棉上预设有定位孔,所述下模对应的定位凸起定位于所述定位孔后,所述上模上通过两个垂直向驱动组件分别固设有对应的第一刀模、第二刀模,所述第一刀模、第二刀模分别独立驱动设置;所述上模板的下端面压装于所述泡棉的上端面,所述上模板上对应于所述第一刀模的刀口、第二刀模的刀口 ...
【技术保护点】
1.一种两孔间距较小的泡棉冲压方法,其特征在于:泡棉的厚度方向设置有两组均布的泡棉孔,分别为第一泡棉孔、第二泡棉孔,所述第一泡棉孔、第二泡棉孔的最小边缘间距不大于1mm,其通过第一刀模整体冲压出第一泡棉孔,之后第一刀模整体上移,通过第二刀模整体冲压出第二泡棉孔,之后第二刀模整体上移。
【技术特征摘要】
1.一种两孔间距较小的泡棉冲压方法,其特征在于:泡棉的厚度方向设置有两组均布的泡棉孔,分别为第一泡棉孔、第二泡棉孔,所述第一泡棉孔、第二泡棉孔的最小边缘间距不大于1mm,其通过第一刀模整体冲压出第一泡棉孔,之后第一刀模整体上移,通过第二刀模整体冲压出第二泡棉孔,之后第二刀模整体上移。2.如权利要求1所述的一种两孔间距较小的泡棉冲压方法,其特征在于:所述泡棉上预设有定位孔,所述下模对应的定位凸起定位于所述定位孔后,所述上模上通过两个垂直向驱动组件分别固设有对应的第一刀模、第二刀模,所述第一刀模、第二刀模分别独立驱动设置...
【专利技术属性】
技术研发人员:吕莉,金民,徐鑫,
申请(专利权)人:苏州安洁科技股份有限公司,
类型:发明