一种平板太阳能集热器板芯卡簧结构制造技术

技术编号:19385972 阅读:53 留言:0更新日期:2018-11-10 00:58
本发明专利技术公开了一种平板太阳能集热器板芯卡簧结构,其特征在于:利用弹簧加工工艺将弹簧钢、高强不锈钢或是工具钢加工为一种卡簧结构,可卡压于板芯结构的吸热板上。该结构广泛适用于平板太阳能集热器板芯结构的固定,可矫正集热器板芯结构的焊接变形,提高平板太阳能集热器的光热转换效率。

Plate core clamping spring structure of flat plate solar collector

The invention discloses a plate core clamping spring structure of a flat solar collector, which is characterized in that the spring steel, high strength stainless steel or tool steel are processed into a clamping spring structure by using the spring processing technology, and can be clamped on the plate core heat absorbing plate. The structure is widely used for fixing the plate core structure of flat panel solar collector. It can correct the welding deformation of the plate core structure of flat panel solar collector and improve the photothermal conversion efficiency of flat panel solar collector.

【技术实现步骤摘要】
一种平板太阳能集热器板芯卡簧结构
在本专利技术涉及平板太阳能集热器领域,尤其是涉及一种平板太阳能集热器板芯固定件。
技术介绍
现有的平板太阳能集热器主要由集热器外壳、保温、集热器板芯、透明盖板等组成,通过分析国内外相关研究与产品试验数据可知集热器的热损系数随着集热器盖板与吸热板之间的间距增大而迅速减小,直到板间距达到10~15mm时达到最小值,间距超过20mm时集热器热损系数继续减小,单减小幅度很小;为控制集热器生产成本,市场上大部分集热器的厚度为70~80mm之间,保温厚度为30mm,铜管直径为20mm,再去除盖板、背板、吸热板等自身厚度共约5mm左右,剩余部分为盖板与吸热板之间的空气间层,其理论间距值为15~20mm之间,但是由于平板太阳能集热器板芯的流道与吸热板在焊接加工的过程中会产生焊接变形,变形量为5~10mm之间;这样会使集热器在组装完成后吸热板与盖板之间的实际间距变小为10mm左右,这严重影响了集热器的热损系数,降低了平板太阳能集热器的光热转换效率。
技术实现思路
本专利技术的目的是,针对现有技术的不足,提供一种平板太阳能板芯卡簧结构,用以矫正平板太阳能集热器板芯的流道与吸本文档来自技高网...

【技术保护点】
1.一种平板太阳能集热器板芯卡簧结构,其特征在于:利用弹簧加工工艺将弹簧钢、高强不锈钢或是工具钢加工为一种卡簧结构。

【技术特征摘要】
1.一种平板太阳能集热器板芯卡簧结构,其特征在于:利用弹簧加工工艺将弹簧钢、高强不锈钢或是工具钢加工为一种卡簧结构。2.根据权利要求1所述的平板太阳能集热器板芯卡簧结构...

【专利技术属性】
技术研发人员:韩荣涛苏万振马斌蔡勇志
申请(专利权)人:德州金亨新能源有限公司
类型:发明
国别省市:山东,37

网友询问留言 已有0条评论
  • 还没有人留言评论。发表了对其他浏览者有用的留言会获得科技券。

1