The invention relates to a preparation method of a chalk, in particular a preparation method of a color pattern chalk. It includes the following steps: gypsum powder 6, titanium dioxide, zinc stearate, 1 copies of 1 copies, 2 copies of polypropylene glycol, paraffin oil, 1 calcium oxide 1 copies, 6 copies of water mixed with homogenizer crushing into slurry, adding emulsifier at 40 DEG C for 30 minutes, cooling to room temperature. Injection mold, the chalk color pattern printed on the periphery of the screen printing method by pressing and drying after release. The invention has the advantages of simple process, few chalk dust and beautiful appearance, so it is very suitable for children's toys.
【技术实现步骤摘要】
彩色花纹粉笔的制备方法
本专利技术涉及一种粉笔的制备方法,具体地说是一种彩色花纹粉笔的制备方法。
技术介绍
粉笔是一种教学用具,一般用于在黑板上使用。但是现在粉笔越来越多作为一种玩具供学龄前儿童玩耍,因此粉笔的外观和色彩也要求越来越高。现有粉笔的制备方法,一般是将粉笔的混合料注入模具内经过冷却、压制、脱模、剪切、干燥而成。因此现有的粉笔形状和色彩都比较单一,不能够满足广大儿童和家长的需求。
技术实现思路
本专利技术的目的就是针对现有粉笔的缺陷,提供一种彩色花纹粉笔的制备方法。本专利技术的技术方案是这样实现的:它包括以下步骤:将石膏粉6份、钛白粉1份、硬脂酸锌1份、聚丙烯醇2份、石蜡油1份、纳米氧化钙1份、水6份混合均匀,用均质机粉碎成浆料,加入乳化剂在40℃保温30分钟,冷却至常温,注入模具,压制成型,采用冲压的方式脱模后采用网印的方法在粉笔外围印上彩色花纹,然后干燥成型。本专利技术工艺方法简单,制备出的粉笔粉尘少,外观漂亮,非常适合作为儿童玩具。具体实施方式以下结合实施例对本专利技术做进一步描述:本专利技术是将石膏粉6份、钛白粉1份、硬脂酸锌1份、聚丙烯醇2份、石蜡 ...
【技术保护点】
一种彩色花纹粉笔的制备方法,它包括以下步骤:将石膏粉6份、钛白粉1份、硬脂酸锌1份、聚丙烯醇2份、石蜡油1份、纳米氧化钙1份、水6份混合均匀,用均质机粉碎成浆料,加入乳化剂在40℃保温30分钟,冷却至常温,注入模具,压制成型,采用冲压的方式脱模后采用网印的方法在粉笔外围印上彩色花纹,然后干燥成型。
【技术特征摘要】
1.一种彩色花纹粉笔的制备方法,它包括以下步骤:将石膏粉6份、钛白粉1份、硬脂酸锌1份、聚丙烯醇2份、石蜡油1份、纳米氧化钙1份、水6份混合均匀,用均...
【专利技术属性】
技术研发人员:邹华军,
申请(专利权)人:应城市君盛石膏制品有限公司,
类型:发明
国别省市:湖北,42