The invention relates to a self sealing hollow wall winding pipe forming method, produced the first tubular body, then making corrugated body, finally winding tube type corrugated body to outside the main body forming a hollow wall winding pipe, corrugated body according to each body required winding length L, in the production of corrugated body, every L produced a solid corrugated body segment, and then in the corrugated tube type winding body to outside the body, cut off the corrugated body located in corrugated solid body segment. It uses interval to set up solid corrugated section, so that when making hollow wall winding pipe, it only needs to cut according to the interval distance of solid corrugated section, and the cutting part is solid corrugated section, no need for additional sealing, simple processing and reliable sealing.
【技术实现步骤摘要】
自密封中空壁缠绕管成型方法
本专利技术涉及缠绕管的
,具体涉及一种自密封中空壁缠绕管成型方法。
技术介绍
中空壁缠绕管由管型的本体和缠绕在本体外部的波纹体构成。其中波纹体为中空结构,在制作完成中空壁缠绕管后,波纹体的两端需要进行密封,以防止在中空壁缠绕管使用时,有水或砂石进入波纹体内部。目前通常的做法是在中空壁缠绕管制作完成后,采用另外制作的与波纹体内腔相配合的堵头将波纹体的两端堵上,以实现密封。上述的制作方式不仅加工复杂、操作繁琐,而且堵头不能保证波纹体两端的绝对密封。
技术实现思路
为解决上述问题,本专利技术的目的在于提供一种加工简单、密封可靠的自密封中空壁缠绕管成型方法。为实现上述目的,本专利技术采取的技术方案为:自密封中空壁缠绕管成型方法,首先制作管型本体,然后制作波纹体,最后将波纹体缠绕至管型本体外部形成中空壁缠绕管,根据每根本体上所需缠绕的波纹体的长度L,在制作波纹体时,每间隔L制作一段实心波纹体段,然后在波纹体缠绕至管型本体外部后,切断波纹体的位置位于实心波纹体段中。本专利技术中的自密封中空壁缠绕管成型方法进一步设置为:所述实心波纹体段 ...
【技术保护点】
自密封中空壁缠绕管成型方法,首先制作管型本体,然后制作波纹体,最后将波纹体缠绕至管型本体外部形成中空壁缠绕管,其特征在于:根据每根本体上所需缠绕的波纹体的长度L,在制作波纹体时,每间隔L制作一段实心波纹体段,然后在波纹体缠绕至管型本体外部后,切断波纹体的位置位于实心波纹体段中。
【技术特征摘要】
1.自密封中空壁缠绕管成型方法,首先制作管型本体,然后制作波纹体,最后将波纹体缠绕至管型本体外部形成中空壁缠绕管,其特征在于:根据每根本体上所需缠绕的波纹体的长度L,在制作波纹体时,每间隔L制作一段实心波纹体段,然后在波纹体缠绕至管型本体外部后,切断波纹体的位置位于实心波纹体段中。2.如权利要求...
【专利技术属性】
技术研发人员:谈刚强,陈鹤忠,
申请(专利权)人:张家港市亿利机械有限公司,
类型:发明
国别省市:江苏,32