The invention discloses a method for improving selection index of high sulfur iron ore mixed red magnetic beneficiation method, will be the first stage of grinding - flotation of sulfur - magnetic separation process, from weak magnetic tailings, obtain sulfur concentrate and concentrate on magnet qualified; weak magnetic separation tailings are discharged into strong magnetic separation apart from the strong magnetic separation tailings T1, obtain strong magnetic concentrate; strong magnetic concentrate to get into fine screening work, sieve products directly as T2 except throwing tailings; fine sieve products into the spiral concentrator process, spiral chute the gravity separation process using a spiral chute roughing, a spiral chute selected spiral concentrator tailings, throw T3, obtain the spiral concentrator iron concentrate C. The present invention has the advantages of high TFe grade, high recovery rate, simple process, stable index, easy operation and management in the field.
【技术实现步骤摘要】
一种提高高硫磁-赤混合铁矿石选别指标的选矿方法
本专利技术属于铁矿石选矿
,具体涉及一种高硫磁-赤混合铁矿石的选矿方法,特别适合于改善原矿TFe品位在35.0%-40.0%范围、赤铁矿之铁占全铁比例在20%-25%之间的高硫磁-赤混合铁矿石的选别指标。
技术介绍
高硫磁-赤混合铁矿石中工业铁矿物主要是磁铁矿,次为赤铁矿等。综合利用的主要矿物为黄铁矿,脉石矿物主要是透辉石、长石、石英、硬石膏等。矿石结构以自形-半自形晶结构为主,其次有它形晶状结构、交代假象结构、交代网状或网脉状结构和交代残余结构。矿石构造以致密块状为主,其次为浸染状构造、网状、网脉状构造和斑杂状构造。黄铁矿呈自形-半自形晶为主,其最大粒径为1.5mm,最小为0.005mm,一般粒径多为0.30~0.01mm。磁铁矿主要呈自形-半自形晶致密块状和网状、网脉状集合体与脉石共生。其最大粒径为10.00mm,最小为0.01mm,一般粒径为0.10~1.50mm。赤铁矿工艺粒度在0.05-0.50mm之间,最大>1.20m,最小为<0.005mm。磁铁矿嵌布粒度粗而赤铁矿嵌布粒度细,给选矿工艺流程的确定 ...
【技术保护点】
一种提高高硫磁‑赤混合铁矿石选别指标的选矿方法,将原矿TFe品位在35.0%‑40.0%范围、赤铁矿之铁占全铁比例在20%‑25%之间、S品位在5.0%~8.0%之间的高硫磁‑赤混合铁矿石,先经阶段磨矿—浮选选硫—弱磁选流程,排出弱磁选尾矿,获得合格的硫精矿及磁铁精矿产品,其特征在于还采用以下工艺、步骤:1)对排出的弱磁选尾矿进行强磁选,抛除强磁选尾矿T1,获得强磁粗精矿;2)对步骤1)获得的强磁粗精矿给入细筛筛分作业,筛上产品直接作为尾矿T2抛除,获得细筛筛下产品;3)对步骤2)获得的细筛筛下产品给入螺旋溜槽重选工艺,所述的螺旋溜槽重选工艺采用一次螺旋溜槽粗选、一次螺旋溜 ...
【技术特征摘要】
1.一种提高高硫磁-赤混合铁矿石选别指标的选矿方法,将原矿TFe品位在35.0%-40.0%范围、赤铁矿之铁占全铁比例在20%-25%之间、S品位在5.0%~8.0%之间的高硫磁-赤混合铁矿石,先经阶段磨矿—浮选选硫—弱磁选流程,排出弱磁选尾矿,获得合格的硫精矿及磁铁精矿产品,其特征在于还采用以下工艺、步骤:1)对排出的弱磁选尾矿进行强磁选,抛除强磁选尾矿T1,获得强磁粗精矿;2)对步骤1)获得的强磁粗精矿给入细筛筛分作业,筛上产品直接作为尾矿T2抛除,获得细筛筛下产品;3)对步骤2)获得的细筛筛下产品给入螺旋溜槽重选工艺,所述的螺旋溜槽重选工艺采用一次螺旋溜槽粗选、一次螺旋溜槽精选,抛出螺旋溜槽重选尾矿T3,获得螺旋溜槽重选铁精矿C。2.如权利要求1所述的一种提高高硫磁-赤混合铁矿石选别指标的选矿方法,其特征在于:步骤1)中强磁选采用的磁选设备为立环脉动高梯度强磁选机,磁场强度采用0.38~0.5T。3.如权利要求1...
【专利技术属性】
技术研发人员:刘军,丁开振,李亮,杨任新,王炬,袁启东,张永,常鲁平,陈洲,李俊宁,
申请(专利权)人:中钢集团马鞍山矿山研究院有限公司,
类型:发明
国别省市:安徽,34