The invention belongs to the technical field of titanium chemical engineering, in particular to a recovery and utilization method of a distillation kettle residual liquid in the process of refining a crude four titanium chloride. The technics of the present invention includes: A, NaCl hybrid, distillation residue and deliquescence crude four titanium chloride refining obtained after hydrolysis, hydrolysis was B, hydrolysis of mud; mud a step of hydrolysis sedimentation after 5 ~ 30h, the upper and lower supernatant was precipitated; C, will lower B step precipitation evaporation the collection of steam and condensation will be condensed after the settlement, have clear liquid and bottom liquid; D, C and B solution steps are steps to get the upper clear liquid mixed again, sedimentation, the supernatant liquid, a two distillation and distillation, refined TiCl
【技术实现步骤摘要】
粗四氯化钛的精制过程蒸馏釜残液的回收利用方法本申请是申请日为:“2016.01.25”,申请号为:“201610049356.3”,申请人为:攀枝花学院,公开号为:“CN105753042A”,专利技术名称为:“粗四氯化钛的精制水解工艺”的分案申请。
本专利技术属于钛化工
,具体涉及一种粗四氯化钛精制过程中蒸馏釜残液的回收利用方法。
技术介绍
TiCl4既是海绵钛生产过程中的重要中间产品,也是氯化法钛白生产环节中的关键性中间环节,高钛渣或人造金红石在氯化炉经过氯气氯化后,得到TiCl4和氯化钙、氯化镁、氯化铁等氯化物组成的混合炉气,混合炉气经收尘、冷凝后获得液态的粗TiCl4,粗TiCl4再进一步蒸馏、精馏,获得精TiCl4产品,精TiCl4通过还原蒸馏可制取海绵钛,通过氧化炉氧化则可生产出氯化钛白。攀枝花某钛业公司2009年建成1.6万t/a规模的TiCl4生产厂,攀钢海绵钛厂已建成1.5万t/a规模的海绵钛生产线,钢城集团公司的海绵钛生产规模达0.5万t/a,攀钢钛业公司10万t/a氯化钛白一期工程项目已破土动工,钛海科技公司选址米易一枝山工业园区的氯化 ...
【技术保护点】
粗四氯化钛的精制过程蒸馏釜残液的回收利用方法,其特征在于:包括以下步骤:a、将粗四氯化钛精制后得到的蒸馏釜残液与潮解的NaCl混合,水解,得水解泥浆;其中,按照重量比,残液TiCl
【技术特征摘要】
1.粗四氯化钛的精制过程蒸馏釜残液的回收利用方法,其特征在于:包括以下步骤:a、将粗四氯化钛精制后得到的蒸馏釜残液与潮解的NaCl混合,水解,得水解泥浆;其中,按照重量比,残液TiCl4:潮解的NaCl=150:12~48;b、将a步骤水解后的水解泥浆沉降5~30h,得上部清液和下部沉淀;c、将b步骤得到的下部沉淀进行蒸发,收集蒸汽并冷凝,将冷凝后的冷凝液进行沉降处理,得清液和底液;d、将c步骤得到的清液与b步骤得到的上部清液混合,再次沉降,取上层清液,进行一级蒸馏和二级精馏,得精制TiCl4;e、将c和d步骤沉降得到的...