Rotating anode plate forming disk of crude copper refining furnace

The utility model relates to a rotating anode plate shaped plate of a crude copper refining furnace, which is a crude copper refining furnace. The utility model has the technical proposal that the utility model is characterized in that the inner edge of the bottom edge of the anode plate groove is provided with an inner bulge, and the edge of the anode plate is avoided. The beneficial effect of this technology is mainly aimed at the anode plate at the bottom edge horn shaped convex set anode plate groove, not only avoid the anode plate edge burr, also disguised in the horn bending portion formed convex, the convex strips can be used directly in the electrolytic tank and the conductive body without obstructing electrolysis, greatly saves the integer time, improve work efficiency.

【技术实现步骤摘要】

本技术涉及电解铜领域中的粗铜精炼后期的一种粗铜精炼炉旋转阳极板定型盘。
技术介绍
在电解铜领域,精铜的精炼是生产阳极板的重要工序,产生的阳极板通过电解产生电解铜,现有的阳极板定型盘为盘体通过转轴旋转,盘体内设有阳极板凹槽,因铜液在流入定型盘的时间很快,阳极板边缘定型不规则,产生毛刺多,尤其是羊角部分,因空间小更不易成型,且在阳极板脱槽时需要从羊角处翘起,因此羊角不仅易变形,毛刺还多,如不整型处理,无法进入电解槽。
技术实现思路
针对上述技术存在的不足,申请人研发出一种无需整型、且边缘无毛刺的粗铜精炼炉旋转阳极板定型盘。技术方案:包括盘体、阳极板槽及盘体中心的转轴,其特征是:所述阳极板槽的底部边缘设置内凸起,避免了阳极板边缘毛刺。有益效果:本技术主要是针对阳极板羊角定型,在阳极板槽的底部边缘设置内凸起,不仅避免了阳极板边缘毛刺,还变相的在羊角弯曲部形成凸起条,此凸起条可直接用于电解槽内与导电体无隔断电解,大大节约了整型时间,提高了工作效率。附图说明:附图1是本实施例中仅画出一个阳极板槽的结构示意图,图中3是阳极板羊角。具体实施方式参照附图1,本实施例主要包括盘体1、阳极板槽2及盘体中心的转轴5,所述阳极板槽2的底部边缘设置内凸起4,避免了阳极板边缘毛刺。

【技术保护点】
粗铜精炼炉旋转阳极板定型盘,包括盘体、阳极板槽及盘体中心的转轴,其特征是:所述阳极板槽的底部边缘设置内凸起。

【技术特征摘要】
1.粗铜精炼炉旋转阳极板定型盘,包括盘体、阳极板槽及盘体...

【专利技术属性】
技术研发人员:朱振祥张俊杰
申请(专利权)人:东营金玺铜业有限公司
类型:新型
国别省市:山东;37