The utility model discloses a demoulding mechanism of a powder pressing forming machine, which comprises a lower mold (5), a lower mold base (2) and a upper mold (1); the utility model also comprises an internal mold (4), the outer wall of the internal mold (4) is slidably connected with the lower mold base (2), the lower mold (5) is slidably connected with the internal mold (4), and a mold cavity (6) is formed between the lower mold (5) and the internal mold (4), and the upper mold (1) is directly above the mold cavity (6) and is slidably connected with the mold during pressing In the cavity (6), the inner wall of the internal mold (4) is tightly matched with the side wall of the lower mold (5) during pressing, and the inner wall of the internal mold (4) is detached from the side wall of the lower mold (5) during opening. After adopting the above structure, the inner wall of the internal mold is separated from the lower mold when opening the mold, so that the pressed product is not adhered by the inner wall of the internal mold, which is more convenient for the ejection of the lower mold; therefore, the qualification rate of the product is greatly improved.
【技术实现步骤摘要】
粉末压制成形机的脱模机构
本技术涉及机械制造设备
,具体讲是一种台粉末压制成形机的脱模机构。
技术介绍
粉末压制成形,是在压模中利用外加压力的成形方法,它的压制成形过程包括装粉、压制和脱模。传统的粉末压制成形机的脱模结构,在导向机构的作用下,下模往上顶,从而把已经压制成形的产品从模腔中顶出。但是,这种结构的粉末压制成形机的脱模机构存在的问题是:第一,由于在压制成形的过程中,粉末很容易粘连在模腔内壁上,一旦外力作用将产品从模腔中顶出,极易发生产品表面破损的现象,因此,产品的合格率低下;第二,考虑到保证合格率的情况下,每一次开模后都要对模腔内壁进行处理,这样一来,脱模效率非常低下,大大降低生产效率。
技术实现思路
本技术所要解决的技术问题是,提供一种既能大大提高产品合格率,又能提高生产效率的粉末压制成形机的脱模机构。为解决上述技术问题,本技术提供的粉末压制成形机的脱模机构,包括下模、下模座和上模;它还包括内模,内模的外侧壁与下模座滑动连接,下模滑动连接在内模中,并且下模和内模之间形成模腔,上模位于模腔的正上方并在压制时滑动连接在模腔内;压制时内模内侧壁与下模的侧壁紧配合,开模时内模的内侧壁与下模的侧壁脱开。所述的内模包括至少两个单元内模块,每个单元内模块的外侧壁与下模座滑动配合,开模时内模的内孔径大于合模时内模的内孔径。所述的单元内模块为三块,沿圆周方向均布。所述下模座与内模的配合面为锥面,相应的内模的外侧壁也为锥面,内模在压制时滑动至下模座底部并与下 ...
【技术保护点】
1.一种粉末压制成形机的脱模机构,包括下模(5)、下模座(2)和上模(1);其特征在于:它还包括内模(4),内模(4)的外侧壁与下模座(2)滑动连接,下模(5)滑动连接在内模(4)中,并且下模(5)和内模(4)之间形成模腔(6),上模(1)位于模腔(6)的正上方并在压制时滑动连接在模腔(6)内;压制时内模(4)内侧壁与下模(5)的侧壁紧配合,开模时内模(4)的内侧壁与下模(5)的侧壁脱开。/n
【技术特征摘要】
1.一种粉末压制成形机的脱模机构,包括下模(5)、下模座(2)和上模(1);其特征在于:它还包括内模(4),内模(4)的外侧壁与下模座(2)滑动连接,下模(5)滑动连接在内模(4)中,并且下模(5)和内模(4)之间形成模腔(6),上模(1)位于模腔(6)的正上方并在压制时滑动连接在模腔(6)内;压制时内模(4)内侧壁与下模(5)的侧壁紧配合,开模时内模(4)的内侧壁与下模(5)的侧壁脱开。
2.根据权利要求1所述的粉末压制成形机的脱模机构,其特征在于:所述的内模(4)包括至少两个单元内模块,每个单元内模块的外侧壁与下模座(2)滑动配合,开模时内模(4)的内孔径大于压制时内模(4)的内孔径。
3.根据权利要求2所述的粉末压制成形机的脱模机构,其特征在于:所述的单元内模块为三块,沿圆周方向均布。
4.根据权利要求1所述的粉末压制成形机的脱模机构,其特征在于:所述下模座(2)与内模(4)的配合面为锥面,相应的内模(4)的外侧壁也为锥面,内模(4)在压制时滑动至下模座(2)底部并与下模(5)紧配,内模(4)在开模时滑动至下模座(2)顶部并与下模(5)脱开。
5.根据权利要求1所述的粉末压制成形机的脱模机构,其特征在于:该脱模机构还包括压板(3...