The invention provides a formulation method of mineral element composition, which comprises a variety of mineral elements and matrices, including 58% silicon, 25% aluminium, 0.5% iron, 0.2% calcium, 0.1% magnesium, 9% potassium, 3% sodium, 0.1% thallium, 3% germanium, 1% selenium, 0.01% rhenium, 0.04% dysprosium, 0.02% praseodymium and 0.03% cobalt, in which the matrix acts as the matrix. Combining with the basic substance of mineral elements, the matrix is porcelain stone. The method for preparing mineral element composition can be obtained by water flow and immersion with water purifier in the family. The mineral element composition is non-toxic and harmless, meets the requirement of human mineral elements, and can be supplemented by regular drinking. Fill the human body with mineral elements.
【技术实现步骤摘要】
一种矿物元素组合物制配方法
本专利技术涉及活水、净水
,尤其涉及一种用于活水、净水的矿物元素组合物制配方法。
技术介绍
矿物质水一般以城市自来水为原水,再经过纯浄化加工,添加矿物质,杀菌处理后灌装而成。但是不是所有人都喜欢购买瓶装水或者桶装水,在家庭中矿物质水不容易得到,也有很多人家中准备了活水器或者净水器,基于此本专利技术提供一种矿物元素组合物,该矿物元素组合物用于配合家里的净水器使用,放置在净水器中通过水流动、浸泡得到矿物质水。
技术实现思路
本专利技术一种矿物元素组合物制配方法,包括多种矿物元素和基质,其中矿物元素包括:58%硅、25%铝、0.5%铁、0.2%钙、0.1%镁、9%钾、3%钠、0.1%铊、3%锗、1%硒、0.01%铼、0.04%镝、0.02%镨、0.03%钴,其中的基质作为结合矿物元素的基本物质,所述基质为瓷石。进一步,所述的矿物元素组合物制配方法,包括以下步骤:a)将上述矿物元素按照分量比例混合,盛放在容器中备用;b)将上述步骤得到的混合物,送入粉碎机内进行粉碎,粉碎后的颗粒大小为0.3-1.3mm,粉碎后的矿物元素放入容器中备用;c)将瓷 ...
【技术保护点】
1.一种矿物元素组合物制配方法,其特征在于:包括多种矿物元素和基质,其中矿物元素包括:58%硅、25%铝、0.5%铁、0.2%钙、0.1%镁、9%钾、3%钠、0.1%铊、3%锗、1%硒、0.01%铼、0.04%镝、0.02%镨、0.03%钴,其中的基质作为结合矿物元素的基本物质,所述基质为瓷石。
【技术特征摘要】
1.一种矿物元素组合物制配方法,其特征在于:包括多种矿物元素和基质,其中矿物元素包括:58%硅、25%铝、0.5%铁、0.2%钙、0.1%镁、9%钾、3%钠、0.1%铊、3%锗、1%硒、0.01%铼、0.04%镝、0.02%镨、0.03%钴,其中的基质作为结合矿物元素的基本物质,所述基质为瓷石。2.根据权利要求1所述的矿物元素组合物制配方法,其特征在于:包括以下步骤:a)将上述矿物元素按照分量比例混合,盛放在容器中备用;b)将上述步骤得到的混合物,送入粉碎机内进行粉碎,粉碎后的颗粒大小...
【专利技术属性】
技术研发人员:唐建业,
申请(专利权)人:张家港健医生物科技有限公司,
类型:发明
国别省市:江苏,32