The utility model discloses a direct welding self-adhesive polyurethane enameled copper round wire, which comprises a copper round wire body (1), a polyurethane resin coating (2), a first nylon layer (3), a second nylon layer (4), an aromatic polyamide resin coating (5) and a polyvinyl butyral resin coating (6), and a spiral groove (7) on the surface of the first nylon layer (3). A composite filament (8) is arranged inside, and the composite filament (8) comprises intertwined glass filament and polyester filament. The polyvinyl butyral resin coating (6) comprises three successive coatings of polyvinyl butyral monolayer. The utility model has the characteristics that the bonding fastness can be effectively improved.
【技术实现步骤摘要】
直焊自粘性聚氨酯漆包铜圆线
本技术涉及一种漆包线,特别是一种直焊自粘性聚氨酯漆包铜圆线。
技术介绍
直焊自粘性漆包线一般是在铜圆线本体外表面依次涂覆聚氨酯层和自粘性漆层,来实现直焊和自粘的功能。但是,现有的直焊自粘性漆包线的粘结牢度不强,使用一段时间后接口容易发生开裂脱落现象,从而影响漆包线的正常使用。因此,现有的技术存在着粘结牢度不理想的问题。
技术实现思路
本技术的目的在于,提供一种直焊自粘性聚氨酯漆包铜圆线。本技术具有能够有效改善粘结牢度的特点。本技术的技术方案:直焊自粘性聚氨酯漆包铜圆线,包括铜圆线本体,铜圆线本体外表面依次涂覆有聚氨酯树脂涂层、第一尼龙层、第二尼龙层、芳香族聚酰胺树脂涂层和聚乙烯醇缩丁醛树脂涂层;所述第一尼龙层表面设有螺旋槽,螺旋槽内设有复合纤维丝;所述复合纤维丝包括相互缠绕的玻璃纤维丝和涤纶纤维丝;所述聚乙烯醇缩丁醛树脂涂层包括三层依次涂覆的聚乙烯醇缩丁醛单层。前述的直焊自粘性聚氨酯漆包铜圆线中,所述聚氨酯树脂涂层、第一尼龙层、第二尼龙层、芳香族聚酰胺树脂涂层和聚乙烯醇缩丁醛树脂涂层之间的厚度比例为1:1.2:1:1.8:2。前述的直焊自粘性聚 ...
【技术保护点】
1.直焊自粘性聚氨酯漆包铜圆线,其特征在于:包括铜圆线本体(1),铜圆线本体(1)外表面依次涂覆有聚氨酯树脂涂层(2)、第一尼龙层(3)、第二尼龙层(4)、芳香族聚酰胺树脂涂层(5)和聚乙烯醇缩丁醛树脂涂层(6);所述第一尼龙层(3)表面设有螺旋槽(7),螺旋槽(7)内设有复合纤维丝(8);所述复合纤维丝(8)包括相互缠绕的玻璃纤维丝和涤纶纤维丝;所述聚乙烯醇缩丁醛树脂涂层(6)包括三层依次涂覆的聚乙烯醇缩丁醛单层。
【技术特征摘要】
1.直焊自粘性聚氨酯漆包铜圆线,其特征在于:包括铜圆线本体(1),铜圆线本体(1)外表面依次涂覆有聚氨酯树脂涂层(2)、第一尼龙层(3)、第二尼龙层(4)、芳香族聚酰胺树脂涂层(5)和聚乙烯醇缩丁醛树脂涂层(6);所述第一尼龙层(3)表面设有螺旋槽(7),螺旋槽(7)内设有复合纤维丝(8);所述复合纤维丝(8)包括相互缠绕的玻璃纤维丝和涤纶纤维丝;所述聚乙烯醇缩丁醛树脂涂层(6)包括三层依次涂覆的聚乙烯醇缩丁醛单层。2.根据权利要求1所述的直焊自粘性聚氨酯漆包铜圆线,其特征在于...