The invention discloses a method for increasing the output of extremely lean ore, which includes the following steps: step 1, crushing and screening the raw ore through crushing equipment until the size of the original ore is less than 25 mm; step 2, in step 1, the crushed and screened raw ore is conveyed to the dry magnetic separator for primary separation through conveyor belt, and the dry concentrate with iron grade more than 12% and the tailings with iron grade less than 12% are selected; Step 3, the dry concentrate selected in step 2 is fed to the high-pressure roller mill for grinding, grinding to the original ore size less than 5mm, then to the wet magnetic separator for cleaning, and the finished concentrate with iron grade more than 28% is selected. Step 4, the dry tailings selected in step 2 are fed to the vibrating screen for screening, and the upper material is fed into the stone production workshop to make the stone, and the lower part of the screen is fed into the conveying device. Wet magnetic separator is used to select concentrate with iron grade (> 28%). The invention separates raw ore to the greatest extent, and improves the mineral yield of extremely lean ore.
【技术实现步骤摘要】
一种提高极贫矿矿产量的方法
本专利技术属于铁矿分选
,尤其涉及一种提高极贫矿矿产量的方法。
技术介绍
我国幅员辽阔,地大物博,矿产资源丰富,西昌地区的钒钛资源丰富,其表外矿和极贫矿储量丰富,合计储量占总可开采量的33.7%,约11184万吨,极贫矿的原矿石品位较低,一般在20%左右,含铁量较低,目前传统工艺主要是针对品位较高的原矿石,对于品位较低的极贫矿原矿石的处理,目前尚无简洁且回收率高的富集方法,无法有效提高极贫矿中的矿产量。
技术实现思路
针对上述现有技术的不足,本专利技术所要解决的技术问题是:如何提供一种简单高效的能够提高极贫矿矿产量的方法。为了解决上述技术问题,本专利技术采用了如下的技术方案:一种提高极贫矿矿产量的方法,包括以下步骤:步骤1,通过破碎设备对原矿石进行破碎再筛分,直至原矿石粒度≤25mm;步骤2,步骤1中破碎筛分后的原矿石通过输送带输送至干式磁选机进行初选,选出铁品位≥12%的干选精矿和铁品位<12%的干选尾矿;步骤3,将步骤2中选出的干选精矿给入高压辊磨机进行磨碎,磨碎至原矿石粒度≤5mm,再给入到湿式磁选机进行精选,选出铁品位≥28% ...
【技术保护点】
1.一种提高极贫矿矿产量的方法,其特征在于,包括以下步骤:步骤1, 通过破碎设备对原矿石进行破碎再筛分,直至原矿石粒度≤25mm;步骤2,步骤1中破碎筛分后的原矿石通过输送带输送至干式磁选机进行初选,选出铁品位≥12%的干选精矿和铁品位<12%的干选尾矿;步骤3,将步骤2中选出的干选精矿给入高压辊磨机进行磨碎,磨碎至原矿石粒度≤5mm,再给入到湿式磁选机进行精选,选出铁品位≥28%的成品精矿;步骤4,将步骤2中选出的干选尾矿给入振动筛进行筛分,筛上物进入石料制作车间制成石料,筛下物通过输送装置进入湿式磁选机进行精选,选出铁品位≥28%的成品精矿,其中所述筛下物粒度≤5mm,筛上物粒度>5mm。
【技术特征摘要】
1.一种提高极贫矿矿产量的方法,其特征在于,包括以下步骤:步骤1,通过破碎设备对原矿石进行破碎再筛分,直至原矿石粒度≤25mm;步骤2,步骤1中破碎筛分后的原矿石通过输送带输送至干式磁选机进行初选,选出铁品位≥12%的干选精矿和铁品位<12%的干选尾矿;步骤3,将步骤2中选出的干选精矿给入高压辊磨机进行磨碎,磨碎至原矿石粒度≤5mm,再给入到湿式磁选机进行精选,选出铁品位≥28%的成品精矿;步骤4,将步骤2中选出的干选尾矿给入振动筛进行筛分,筛上物进入石料制作车间制成石料,筛下物通过输送装置进入湿式磁选机进行精选,选出铁品位≥28%的成品精矿,其中所述筛下物粒度≤5mm,筛上物粒度>5mm。2.根据权利要求1所述的一种提高极贫矿矿产量的方法,其特征在于:所述振动筛下方设置有水槽,所述筛下物进入水槽中形成矿浆,并通过所述输送装置输送到所述湿式磁选机进行精选。3.根据权利要求2所述的一种提高极贫矿矿...