The invention discloses a method for separating fluorite from rare earth tailings, which belongs to the technical field of mineral processing engineering. The method includes mixed flotation, fluorite one roughness seven fine flotation, magnetic separation, one roughness two fine shaking bed gravity separation, and finally a fluorite concentrate with 95% CaF2 grade can be obtained. Through the mineral processing method provided by the invention, the fluorite resources in the rare earth tailings of Bayan Obo beneficiation can be recovered to produce high quality fluorite concentrate, which has high economic value and great significance for environmental protection.
【技术实现步骤摘要】
一种稀土尾矿中分选萤石的方法
本专利技术属于选矿工程
,具体涉及一种稀土尾矿中分选萤石的方法。
技术介绍
我国的萤石资源,除了单一的萤石矿之外,还有许多伴生萤石资源。白云鄂博矿萤石储量十分巨大,属伴生矿床,CaF2含量较低。白云鄂博氧化矿选出铁、稀土后的尾矿中萤石得到富集,CaF2含量在20-25%左右,所含矿物种类较多,共生关系复杂,嵌布粒度较细,其中所含主要脉石矿物与萤石物理化学性质十分相近,给选矿造成很大困难。随着白云鄂博氧化矿尾矿中综合回收铁、稀土选矿技术的日益成熟,国家对资源综合利用的要求,新兴产业对高品位萤石需求的不断增加,白云鄂博矿萤石资源回收日益重要。除具有明显价值外,萤石资源的回收有效避免资源浪费,以及尾矿中含氟资源对土地的污染,有很好社会效益。目前,以包钢矿山研究院专利技术专利《一种从稀土尾矿中综合回收利用多种矿产资源的选矿工艺》(专利号为ZL201410319762.8)为基础,白云鄂博宝山矿业公司萤石生产线已经按照该专利进行设计并建成调试,但是由于原矿性质与小型试验时发生改变,逐渐由氧化矿转为磁矿,同时,在现场前一阶段稀土尾矿无法降低 ...
【技术保护点】
1.一种稀土尾矿中分选萤石的方法,其特征在于,所述方法包括以下步骤:S1:混合浮选采用一粗两精浮选工艺对稀土尾矿进行混合浮选,浮选浓度大于40%,得到CaF2品位50%以上混合浮选精矿;S2:萤石浮选采用一粗七精浮选工艺对混合浮选精矿进行萤石浮选,浮选浓度为40‑50%,pH值为6.3‑6.7,得到CaF2品位86%以上萤石浮选精矿;S3:磁选采用磁场对萤石浮选精矿进行磁选,得到CaF2品位88%以上萤石磁选精矿;S4:摇床重选采用一粗两精重选工艺对萤石磁选精矿进行摇床重选,得到CaF2品位大于95%的萤石精矿。
【技术特征摘要】
1.一种稀土尾矿中分选萤石的方法,其特征在于,所述方法包括以下步骤:S1:混合浮选采用一粗两精浮选工艺对稀土尾矿进行混合浮选,浮选浓度大于40%,得到CaF2品位50%以上混合浮选精矿;S2:萤石浮选采用一粗七精浮选工艺对混合浮选精矿进行萤石浮选,浮选浓度为40-50%,pH值为6.3-6.7,得到CaF2品位86%以上萤石浮选精矿;S3:磁选采用磁场对萤石浮选精矿进行磁选,得到CaF2品位88%以上萤石磁选精矿;S4:摇床重选采用一粗两精重选工艺对萤石磁选精矿进行摇床重选,得到CaF2品位大于95%的萤石精矿。2.根据权利要求1所述的方法,其特征在于,步骤S1中,所述一粗两精浮选工艺中采用酸化水玻璃作为pH调整剂,用量为1.0-1.3kg/t。3.根据权利要求1所述的方法,其特征在于,步骤S1中,所述一粗两精浮选工艺中采用脂肪酸类捕收剂SF作为捕收剂,...
【专利技术属性】
技术研发人员:李宏静,刘春光,贾佳,王丽明,刘涛,白春霞,王海洲,李燕,
申请(专利权)人:包头钢铁集团有限责任公司,
类型:发明
国别省市:内蒙古,15