The invention relates to the technical field of mineral processing, in particular to a mineral processing method for breccia lead-zinc sulfide ore using backwater. After grinding, adding pulp pH regulator lime, galena collector 25 # black powder, sphalerite collector butyl xanthate for one lead roughing and two lead scavenging, lead crude concentrate and lead scavenging tailings were obtained. Lead crude concentrate was added with deactivating activated carbon, sphalerite inhibitor zinc sulfate and 25 # black powder for three lead concentrating and two lead scavenging, and lead concentrate and lead concentrate tailings were obtained. Zinc concentrate is obtained by merging the cleaning tailings with lead concentrate, adding lime, activator copper sulfate, collector butyl xanthate, foaming agent terpineol oil for one zinc roughing, two zinc sweeping, three zinc concentrating and two zinc concentrating. Zinc sweeping tailings and concentrating tailings are merged into final tailings. The method of the invention has the advantage that the mineral processing backwater can be directly reused without treatment, and good lead-zinc beneficiation indexes can be obtained under the condition of using backwater.
【技术实现步骤摘要】
一种回水直接可用的角砾岩型硫化铅锌矿选矿方法
本专利技术涉及选矿
,特别是涉及一种回水直接可用的角砾岩型硫化铅锌矿选矿方法。
技术介绍
选矿过程需要消耗大量水,如何利用回水、且不对选矿指标造成过大影响,是选矿技术人员在开发选矿工艺时需要考虑的重要问题。目前在选矿回水利用方面,国内常用自然降解、混凝沉淀、中和、吸附和氧化分解等方法处理。目前国内硫化铅锌矿选矿普遍采用两种回水利用工艺,一是混合废水深度处理后回用;二是适度处理后分质回用。例如栖霞铅锌矿选矿采用适度处理-分质回用的方法对回水进行利用,具体是选硫尾矿回水回用至选硫作业,部分锌尾矿浓缩回水回用至选锌作业,铅锌精矿及剩余锌尾矿浓缩回水采用混凝沉淀-吸附处理后回用至磨矿选铅作业。会泽铅锌矿是采用沉钙镁-絮凝沉降-吸附,之后再集中回用。混合废水深度处理回用具有废水处理规模大、工艺复杂、成本高等缺点;而适度处理-分质回用需建铅尾矿浓缩系统,一次性基建投资大,并且使用回水后铅锌选矿指标很不稳定。现有的硫化铅锌矿选矿回水不能直接回用的原因主要是在硫化铅锌矿浮选分离中添加了不同类型的捕收剂和闪锌矿活化剂,在回水中含有 ...
【技术保护点】
1.一种回水直接可用的角砾岩型硫化铅锌矿选矿方法,其特征在于,包括以下步骤:S1:角砾岩型硫化铅锌矿磨矿将角砾岩型硫化铅锌矿原矿磨细至‑0.075mm质量百分比含量占50~72%,得到原矿磨矿产品;S2:铅粗选原矿磨矿产品进行铅粗选,铅粗选作业的工艺条件为:按角砾岩型硫化铅锌矿原矿质量计,首先添加石灰590~700g/t,作用时间2min,之后再添加丁基黄药0~10g/t、25#黑药8~20g/t,作用时间2min,进行铅粗选,得到的粗选泡沫为铅粗精矿,得到的粗选底流为铅粗尾矿;向所述粗选底流中添加4~5g/t的25#黑药进行铅粗一次扫选,铅粗一次扫选得到的泡沫返回至铅粗选 ...
【技术特征摘要】
1.一种回水直接可用的角砾岩型硫化铅锌矿选矿方法,其特征在于,包括以下步骤:S1:角砾岩型硫化铅锌矿磨矿将角砾岩型硫化铅锌矿原矿磨细至-0.075mm质量百分比含量占50~72%,得到原矿磨矿产品;S2:铅粗选原矿磨矿产品进行铅粗选,铅粗选作业的工艺条件为:按角砾岩型硫化铅锌矿原矿质量计,首先添加石灰590~700g/t,作用时间2min,之后再添加丁基黄药0~10g/t、25#黑药8~20g/t,作用时间2min,进行铅粗选,得到的粗选泡沫为铅粗精矿,得到的粗选底流为铅粗尾矿;向所述粗选底流中添加4~5g/t的25#黑药进行铅粗一次扫选,铅粗一次扫选得到的泡沫返回至铅粗选作业,铅粗一次扫选得到的底流中添加4~5g/t的25#黑药进行铅粗二次扫选,铅粗二次扫选得到的泡沫返回至铅粗一次扫选作业,铅粗二次扫选得到的底流为铅扫选尾矿;S3:铅精选铅粗精矿中首先添加活性炭120~300g/t,作用时间2min,之后添加硫酸锌140~300g/t,作用时间2min,然后添加25#黑药0~16g/t,作用时间2min,进行铅一次精选,得到铅一次精选泡沫和铅一次精选底流,铅一次精选泡沫中添加硫酸锌50~140g/t、25#黑药0~4g/t,进行铅二次精选,得到铅二次精选泡沫和铅二次精选底流,铅二次精选底流返回至铅一次精选作业,铅二次精选泡沫直接进行空白铅三次精选,得到铅三次精选泡沫和铅三次精选底流,得到的铅三次精选底流返回至铅二次精选作业,得到的铅三次精选泡沫为铅精矿;铅一次精选底流中添加25#黑药4~8g/t进行铅精一次扫选,得到铅精一次扫选泡沫和铅精一次扫选底流,铅精一次扫选泡沫返回至铅一次精选作业,铅精一次扫选底流中添加25#黑药0~8g/t进行铅精二次扫选,得到铅精二次扫选泡沫和铅精二次扫选底流,得到的铅精二次扫选泡沫返回至铅精一次扫选作业,得到的铅精二次...