The invention discloses an invention, which specifically relates to a petroleum ether purification process with a boiling range of 90 120. The petroleum ether purification process with a boiling range of 90 120 includes the following steps: step 1, sulfur treatment; step 2: water washing; step 3: alkali washing; the design of the invention is reasonable, and the petroleum ether with a boiling range of 90 120 obtained by the method has high purity, simple and reasonable process, high qualified rate and suitable product. To meet the needs of large-scale industrial production.
【技术实现步骤摘要】
沸程90-120的石油醚提纯工艺
本专利技术涉及化工领域,尤其是涉及沸程90-120的石油醚提纯工艺。
技术介绍
传统的沸程90-120的石油醚制备工艺,在生产过程中多采用98%硫酸处理石油醚,实现高纯度较为困难。
技术实现思路
本专利技术为解决上述提出到的沸程90-120的石油醚纯度不高的问题,为此提供了一种色谱级石油醚制备工艺。本专利技术的技术方案是:一种沸程90-120的石油醚制备工艺,所述沸程90-120的石油醚制备工艺的步骤包括:步骤一,硫处理:采用低含量的发烟硫酸在搅拌和控温时按一定比例加入到工业级沸程90-120的石油醚中;步骤二,水洗:搅拌40分钟,水洗,弃去下部沉降物,得到上层液体;步骤三,碱洗:加水稀释氢氧化钠水溶液,使得其PH值在8左右,碱洗上层液体,去水后留上层清液在氢氧化钠作用下分馏得到色谱级沸程90-120的石油醚。作为优选,所述步骤一中,发烟硫酸与石油醚的质量比为1:8,温度控制在8摄氏度。作为优选,所述步骤三中,氢氧化钠溶液的浓度在40%。本专利技术的有益效果是:本专利技术设计合理,该方法所得沸程90-120的石油醚纯度高,工艺简单合理 ...
【技术保护点】
1.一种沸程90‑120的石油醚提纯工艺,其特征在于:它包括以下步骤:步骤一,硫处理:采用低含量的发烟硫酸在搅拌和控温时按一定比例加入到工业级沸程90‑120的石油醚中;步骤二,水洗:搅拌40分钟,水洗,弃去下部沉降物,得到上层液体;步骤三, 碱洗:加水稀释氢氧化钠水溶液,使得其PH值在8左右,碱洗上层液体,去水后留上层清液在氢氧化钠作用下分馏得到色谱级沸程90‑120的石油醚。
【技术特征摘要】
1.一种沸程90-120的石油醚提纯工艺,其特征在于:它包括以下步骤:步骤一,硫处理:采用低含量的发烟硫酸在搅拌和控温时按一定比例加入到工业级沸程90-120的石油醚中;步骤二,水洗:搅拌40分钟,水洗,弃去下部沉降物,得到上层液体;步骤三,碱洗:加水稀释氢氧化钠水溶液,使得其PH值在8左右,碱洗上层液...